Fire Effect for Carbon Steel Pipes Stress

I need to know how to determine the change of mechanicail proporties for material due to heat effect from fire


 
 Reply 
 
elgazery
Consultant
National Institute for Standards, Egypt, Joined May 2003, 10

elgazery

Consultant
National Institute for Standards,
Egypt,
Joined May 2003
10
00:18 May-18-2004
Re: Fire Effect for Carbon Steel Pipes Stress
the ultrasonic velocity measurements may be efficient in this job.
it depends on :
how and how long this pipes are fired?


 
 Reply 
 
elgazery
Consultant
National Institute for Standards, Egypt, Joined May 2003, 10

elgazery

Consultant
National Institute for Standards,
Egypt,
Joined May 2003
10
00:18 May-18-2004
Re: Fire Effect for Carbon Steel Pipes Stress
the ultrasonic velocity measurements may be efficient in this job.
it depends on :
how and how long this pipes are fired?


 
 Reply 
 

Product Spotlight

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

AMIGO2

TSC Amigo2 - ACFM technology has developed a solid reputation for accurately detecting and sizing
...
surface-breaking cracks through paint and coatings. As the industry demands increased performance in speed, signal quality, and portability, it’s time for an evolution. It’s time for Amigo2.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window