PAUT in Inconel cladding

Hai Experts,
Is PAUT possible for the following joints..

1)Volumetric examination and bond line integrity check in cladded area.

cladded Pipe OD/Material=24"/ API 5L X65
Cladding material & thickness=Inconel 625 & 4.3 mm thickness.
Is there any special Probe like DMA or DLA required?

2)Volumetric Examination in butt joint/similar welds

Butt joint= similar welds ,single 'V' between cladded pipe and cladded hanger flange.

 
 Reply 
 
Aniss Ziani
, Advanced NDT inspector
ISQ, Algeria, Joined Nov 2014, 32

Aniss Ziani

, Advanced NDT inspector
ISQ,
Algeria,
Joined Nov 2014
32
15:12 Mar-11-2017
Re: PAUT in Inconel cladding
In Reply to sreejith at 02:21 Mar-11-2017 (Opening).

Hi Sreejith,
Have a look on this interesting article from Carlo Romito and Frederic Jacques :
https://www.linkedin.com/pulse/method-automatic-ultrasonic-testing-aut-corrosion-resistant-romito-1
Regards,
Aniss Ziani

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 832

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
832
22:24 Mar-11-2017
Re: PAUT in Inconel cladding
In Reply to sreejith at 02:21 Mar-11-2017 (Opening).

what is the weld material ?

 
 Reply 
 
sreejith
India, Joined Jan 2015, 5

sreejith

India,
Joined Jan 2015
5
02:24 Mar-13-2017
Re: PAUT in Inconel cladding
In Reply to Anmol Birring at 22:24 Mar-11-2017 .

SMAW,E7018

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 832

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
832
05:48 Mar-13-2017
Re: PAUT in Inconel cladding
In Reply to sreejith at 02:24 Mar-13-2017 .

So it is carbon steel weld with A625 clad overlay ?

 
 Reply 
 
sreejith
India, Joined Jan 2015, 5

sreejith

India,
Joined Jan 2015
5
07:26 Mar-14-2017
Re: PAUT in Inconel cladding
In Reply to Anmol Birring at 05:48 Mar-13-2017 .

yes

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 832

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
832
04:19 Mar-16-2017
Re: PAUT in Inconel cladding
In Reply to sreejith at 07:26 Mar-14-2017 .

If the weld is CS, you can use PAUT - shear wave but limited to the 1/2 vee mode. So that will mean removal of weld cap to get full weld coverage. And since it is CS you can add TOFD

 
 Reply 
 

Product Spotlight

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window