Cast Steel

I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.

Does anyone have any information on this or sources I can consult?


 
 Reply 
 
emily woo
emily woo
02:28 May-26-2004
Re: Cast Steel
i would like to know the advantages of CAST STEEL AS 2074 Grade C5.

----------- Start Original Message -----------
: I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.
: Does anyone have any information on this or sources I can consult?
------------ End Original Message ------------




 
 Reply 
 
James Dolfi
Director
ford, USA, Joined Oct 1999, 8

James Dolfi

Director
ford,
USA,
Joined Oct 1999
8
00:36 May-27-2004
Re: Cast Steel
----------- Start Original Message -----------
: i would like to know the advantages of CAST STEEL AS 2074 Grade C5.
: : I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.
: : Does anyone have any information on this or sources I can consult?
------------ End Original Message ------------

You may be able to get all the info you want at
http://www.key-to-steel.com/

They cross reference all steels and standards.



 
 Reply 
 
ian
ian
04:16 Jul-21-2004
Re: Cast Steel
thank you so much for this opportunity. i want to know about the chemical compositions of material called GS-60.3 . Thank you


 
 Reply 
 
Ed T.
Ed T.
05:28 Jul-22-2004
Re: Cast Steel
----------- Start Original Message -----------
: thank you so much for this opportunity. i want to know about the chemical compositions of material called GS-60.3 . Thank you
------------ End Original Message ------------
Try these links:

http://www.rz.fh-ulm.de/labore/wplabor/Englisch/FurtherInfo/Tests/Test11/metallographic%20determination%20v11.htm
http://www.felis.hr/en/cast-general.html
http://www.proximedia.com/local/jkservice/produkt1ban.htm


 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

MIZ®-21C: Truly Affordable Eddy Current Handheld with Surface Array Capability

Introducing MIZ-21C, the first truly affordable handheld eddy current instrument with surface array
...
capabilities. MIZ-21C can deliver fast, accurate inspections in demanding NDT applications including aerospace, oil and gas, manufacturing, and power generation. The surface array solution can reduce inspection time by up to 95% compared to traditional handheld pencil probes. The ergonomic design, long battery life, and intuitive touchscreen mean you can inspect more areas faster than ever without fatigue.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Surf-X® Array Probe

Introducing the Surf-X family of flexible Eddy Current Array (ECA) probes. Featuring unique multiple
...
coil sets and proprietary X-PROBE technology, Surf-X array probes can quickly and accurately handle a range of inspection applications, from inspecting corrosion or cracking in pipes, pressure vessels, or tanks, to assessing and sizing cracks in raised welds and friction stir welds.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window