Jim McGregor
Jim McGregor
01:23 Jun-02-2004
Attenuation measurments to check for hydrogen attack

I am looking for information on carrying out attenuation measurments on a 75mm thick carbon steel vessel before and after heat soak to check for hydrogen dispersement. The vessel has been in use for the past 10 years or so. Any help with details and /or a test procedure would be appreciated.

Thanks,

Jim McGregor


 
 Reply 
 
Sasaki
Sasaki
03:34 Jun-02-2004
Re: Attenuation measurments to check for hydrogen attack
There are five methods to detect a certain type of hydrogen attack:
1) flaw echo
2) attenuation
3) frequency analysis
4) sound velocity
5) comparison of longitudinal/transverse sound velocities


 
 Reply 
 
Kasper Pols
Kasper Pols
09:35 Jun-02-2004
Re: Attenuation measurments to check for hydrogen attack
----------- Start Original Message -----------
: I am looking for information on carrying out attenuation measurments on a 75mm thick carbon steel vessel before and after heat soak to check for hydrogen dispersement. The vessel has been in use for the past 10 years or so. Any help with details and /or a test procedure would be appreciated.
: Thanks,
: Jim McGregor
------------ End Original Message ------------

See website: Sensistor



 
 Reply 
 
Jan Verkooijen
Director,
Sonovation, Netherlands, Joined Nov 1998, 29

Jan Verkooijen

Director,
Sonovation,
Netherlands,
Joined Nov 1998
29
04:28 Jun-02-2004
Re: Attenuation measurments to check for hydrogen attack
----------- Start Original Message -----------
: : I am looking for information on carrying out attenuation measurments on a 75mm thick carbon steel vessel before and after heat soak to check for hydrogen dispersement. The vessel has been in use for the past 10 years or so. Any help with details and /or a test procedure would be appreciated.
: : Thanks,
: : Jim McGregor
: See website: Sensistor
------------ End Original Message ------------
Jim,

Detection and monitoring is not a simple subject.
First of all you have to define what type of Hydrogen damage can be expected. Is the vessel operating in high temperature / high pressure environment? In this case you could have High Temperature Hydrogen Attack. Is it working at low temperature, you might be looking at one or more types of Hydrogen Induced Cracking. There is not one method that on its own will give you a conclusive answer on whether you do or don't have Hydrogen Damage. Therefore, during the last 15 years we have developed and practiced combinations of techniques, optimised for the situation at hand. We provide the service worldwide, so if you are interested let us look at your challenge.

Best regards,

Jan Verkooijen



 
 Reply 
 

Product Spotlight

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window