NDT method selection on SS Vessels

Dear All,

Could you all please advise me suitable NDT methods and their detailed specifications for the surface and near surface crack detection of pressure vessels made of made of SS304L and SS316L materials and operating at 65-80 deg. C temperature range

Thanks,

Prasad




 
 Reply 
 
D.Simon Amallraja
D.Simon Amallraja
04:58 May-31-2004
Re: NDT method selection on SS Vessels
----------- Start Original Message -----------
: Dear All,
: Could you all please advise me suitable NDT methods and their detailed specifications for the surface and near surface crack detection of pressure vessels made of made of SS304L and SS316L materials and operating at 65-80 deg. C temperature range
: Thanks,
: Prasad
------------ End Original Message ------------

Dear Mr. Prasad,

Give your complete postal address with telephone nos, so we can contact you and discuss with your requirement. We can also suggest you suitable equipment and guide you.

D.Simon Amallraja.
Asst.Manager -NDT,
Mahindra Intertrade Ltd,
1-7-1,Parklane, Secunderabad - 500003.
Ph: 0 98480 43309.


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 305

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
305
08:23 Jun-01-2004
Re: NDT method selection on SS Vessels
----------- Start Original Message -----------
: Dear All,
: Could you all please advise me suitable NDT methods and their detailed specifications for the surface and near surface crack detection of pressure vessels made of made of SS304L and SS316L materials and operating at 65-80 deg. C temperature range
: Thanks,
: Prasad
------------ End Original Message ------------
Dear Prasad,
Perhaps you could provide some more details for the NDT community out there.
What do you mean by "Near Surface".
What do you want to inspect? Welds and H.A.Z. only or entire vessel?
I assume that the vessel will be at normal temperature and access inside when you want to inspect. Can you please confirm. Also that any necessary insulation will be removed prior to inspection.

Regards,

Godfrey Hands




 
 Reply 
 
R J Chaudhari
Director,
CALTECH ENGINEERING SERVICES, India, Joined Mar 2003, 13

R J Chaudhari

Director,
CALTECH ENGINEERING SERVICES,
India,
Joined Mar 2003
13
03:56 Jun-02-2004
NDT method selection on SS Vessels
Dear Prasad,
Best NDT Method will be Field Metallography. You can confirm not only cracks but also microstructure of pressure vessel without distroying material. You can also get photographs and replicas for your records and expert evaluations, decisions.

Regards,

R J Chaudhari


----------- Start Original Message -----------
: : Dear All,
: : Could you all please advise me suitable NDT methods and their detailed specifications for the surface and near surface crack detection of pressure vessels made of made of SS304L and SS316L materials and operating at 65-80 deg. C temperature range
: : Thanks,
: : Prasad
: Dear Prasad,
: Perhaps you could provide some more details for the NDT community out there.
: What do you mean by "Near Surface".
: What do you want to inspect? Welds and H.A.Z. only or entire vessel?
: I assume that the vessel will be at normal temperature and access inside when you want to inspect. Can you please confirm. Also that any necessary insulation will be removed prior to inspection.
: Regards,
: Godfrey Hands
------------ End Original Message ------------




 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
01:59 Jun-02-2004
Re: NDT method selection on SS Vessels
Prasad,

One of the best "NDT" methods for SS vessels is using ID and OD Creeping Waves. These waves travel along the ID and OD surfaces (longitudinal waves velocities) to detect flaws which are perpendicular to the surfaces.

I have demonstrated detection of ID and OD cracks as small as 0.001 inches in depth.

One concern is the type of SS material. What is the grain size. When the grain size approaches "1" or "O" in size Creeping waves generation on the ID surface may not be generated. What is the thickness?

Another consideration is the carbon content and what type of crack you might be looking for.

For a explanation of ID and OD Creeping Waves go to the publications section of ndt.net and see review The Advanced Ultraosnic Sizing Handbook I wrote.

Sincerely,

J. Mark Davis

----------- Start Original Message -----------
: Dear Prasad,
: Best NDT Method will be Field Metallography. You can confirm not only cracks but also microstructure of pressure vessel without distroying material. You can also get photographs and replicas for your records and expert evaluations, decisions.
: Regards,
: R J Chaudhari
:
: : : Dear All,
: : : Could you all please advise me suitable NDT methods and their detailed specifications for the surface and near surface crack detection of pressure vessels made of made of SS304L and SS316L materials and operating at 65-80 deg. C temperature range
: : : Thanks,
: : : Prasad
: : Dear Prasad,
: : Perhaps you could provide some more details for the NDT community out there.
: : What do you mean by "Near Surface".
: : What do you want to inspect? Welds and H.A.Z. only or entire vessel?
: : I assume that the vessel will be at normal temperature and access inside when you want to inspect. Can you please confirm. Also that any necessary insulation will be removed prior to inspection.
: : Regards,
: : Godfrey Hands
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window