How to design a piezocomposite transducer?

I want to design a 1-3 piezocomposite transducer with 10Mz central frequency and wide bandwidth. But I have not any experience on it. So need your help.
1.Where can I get some technical books which introduce the principle of making transducer and step by step teaching how to make a PZT transducer?
2.how to select the materials of the transducer?
3.how to determine the structure size of the transducer?


 
 Reply 
 
Paul A. Meyer
R & D,
GE Inspection Technologies, USA, Joined Nov 1998, 47

Paul A. Meyer

R & D,
GE Inspection Technologies,
USA,
Joined Nov 1998
47
02:53 Jun-21-2004
Re: How to design a piezocomposite transducer?
Try to get a copy of ULTRASONIC TRANSDUCERS FOR NONDESTRUCTIVE TESTING by M. G. Silk. It was published in 1984 by Adam Hilger Ltd, Bristol. There may be later editions. This book is a comprehensive review of transducer design and operation and also covers piezocomposite materials.
A lierature search should also produce several articles on transducer design.
Paul
----------- Start Original Message -----------
: I want to design a 1-3 piezocomposite transducer with 10Mz central frequency and wide bandwidth. But I have not any experience on it. So need your help.
: 1.Where can I get some technical books which introduce the principle of making transducer and step by step teaching how to make a PZT transducer?
: 2.how to select the materials of the transducer?
: 3.how to determine the structure size of the transducer?
------------ End Original Message ------------




 
 Reply 
 
X. Chen
X. Chen
03:13 Jun-21-2004
Re: How to design a piezocomposite transducer?
Thank you very much for your kindly help. I will try.

----------- Start Original Message -----------
: Try to get a copy of ULTRASONIC TRANSDUCERS FOR NONDESTRUCTIVE TESTING by M. G. Silk. It was published in 1984 by Adam Hilger Ltd, Bristol. There may be later editions. This book is a comprehensive review of transducer design and operation and also covers piezocomposite materials.
: A lierature search should also produce several articles on transducer design.
: Paul
: : I want to design a 1-3 piezocomposite transducer with 10Mz central frequency and wide bandwidth. But I have not any experience on it. So need your help.
: : 1.Where can I get some technical books which introduce the principle of making transducer and step by step teaching how to make a PZT transducer?
: : 2.how to select the materials of the transducer?
: : 3.how to determine the structure size of the transducer?
------------ End Original Message ------------


 
 Reply 
 
arun kumar
arun kumar
04:17 Oct-18-2004
Re: How to design a piezocomposite transducer?

I want to design a 1-3 piezocomposite transducer with 10Mz central frequency and wide bandwidth. But I have not any experience on it. So need your help.
1.Where can I get some technical books which introduce the principle of making transducer and step by step teaching how to make a PZT transducer?
2.how to select the materials of the transducer?
3.how to determine the structure size of the transducer?




 
 Reply 
 

Product Spotlight

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window