Hello,
Does anyone have a suggestion where to find criteria for rejection or approval of defects like nicks, dents or scratches on hardened carbonized raceway surfaces.
I already have ANSI B3.2-1992

thanks
xander


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
05:05 Jul-22-2004
Re: defects on bearingraceways
----------- Start Original Message -----------
: Hello,
: Does anyone have a suggestion where to find criteria for rejection or approval of defects like nicks, dents or scratches on hardened carbonized raceway surfaces.
: I already have ANSI B3.2-1992
: thanks
: xander
------------ End Original Message ------------

Hi Xander,

Many bearing manufacturers will have their own specification for acceptance of nicks, dents and scratches on bearing raceways.
They keep this information proprietary, so it will be very difficult to get information from them.

The main cause of failure from surface breaking features such as you describe are the effect of the hydraulic pressure that the lubricant applies on the raceway as the feature is overrolled. This holds valid also for raceway surface breaking cracks.

For slightly sub-surface defects, a different failure mechanism comes in to play. This is the effect of compressive stresses on the Hertzian zone, and depending on the rolling element diameter can be between several hundredths of a millimetre to a small number of millimetres deep. This means that inclusions in this region are not recommended, and may shorten the bearing life.

I suggest that you request some information from a bearing manufacturer, and offer to hold the information obtained as confidential.

Regards,

Godfrey Hands



 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window