05:22 Jul-20-2004
defects on bearingraceways

Hello,
Does anyone have a suggestion where to find criteria for rejection or approval of defects like nicks, dents or scratches on hardened carbonized raceway surfaces.
I already have ANSI B3.2-1992

thanks
xander


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 304

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
304
05:05 Jul-22-2004
Re: defects on bearingraceways
----------- Start Original Message -----------
: Hello,
: Does anyone have a suggestion where to find criteria for rejection or approval of defects like nicks, dents or scratches on hardened carbonized raceway surfaces.
: I already have ANSI B3.2-1992
: thanks
: xander
------------ End Original Message ------------

Hi Xander,

Many bearing manufacturers will have their own specification for acceptance of nicks, dents and scratches on bearing raceways.
They keep this information proprietary, so it will be very difficult to get information from them.

The main cause of failure from surface breaking features such as you describe are the effect of the hydraulic pressure that the lubricant applies on the raceway as the feature is overrolled. This holds valid also for raceway surface breaking cracks.

For slightly sub-surface defects, a different failure mechanism comes in to play. This is the effect of compressive stresses on the Hertzian zone, and depending on the rolling element diameter can be between several hundredths of a millimetre to a small number of millimetres deep. This means that inclusions in this region are not recommended, and may shorten the bearing life.

I suggest that you request some information from a bearing manufacturer, and offer to hold the information obtained as confidential.

Regards,

Godfrey Hands



 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window