MX2 Zone Discrimination

I was told that the Omniscan MX2 supports zone discrimination, this is something new for me and I am learning more about it.

What I know so far is that it needs to be done through Tomoview, but, that´s how far I got.

How to create such setup?

Standard in question is API 1104

 
 Reply 
 
Mohammad.H.Taghipour
Director,
Pars Leading Inspection Company, Iran, Joined Apr 2012, 4

Mohammad.H.Taghipour

Director,
Pars Leading Inspection Company,
Iran,
Joined Apr 2012
4
14:46 Apr-05-2018
Re: MX2 Zone Discrimination
In Reply to Andre Ribeiro at 17:16 Apr-04-2018 (Opening).

Hi buddy

Zonal discrimination technique which cal ( AUT) is based on ASTM E1961 and also DNV OSF-101 for offshore pipeline girth welds inspection.

There is two main equipment's for AUT, RotoScan for Applus RTD & Pipewizard for Olympus.

Omniscan MX2 can't support zonal technique but TD-Handy scan & TD-Handy Scan RX can support zonal technique with automated band type scanner, but can support zonal inspection up to 15 mm thickness ( it's depend on the bevel config )


 
 Reply 
 
Andre Ribeiro
NDT Inspector,
Self Employed, Brazil, Joined Apr 2008, 18

Andre Ribeiro

NDT Inspector,
Self Employed,
Brazil,
Joined Apr 2008
18
15:30 Apr-05-2018
Re: MX2 Zone Discrimination
In Reply to Mohammad.H.Taghipour at 14:46 Apr-05-2018 .

Yeah, I am aware of all that AUT stuff, have done the Rotoscan course, and fidled with the UT Scan system from UT Quality a little bit, also worked with the AGR equipments.

Still, there are people that disagree with the afirmation that the MX2 can´t do zonal.

It just occured me, I´ll ask directly on the source with the Olympus guys.

Thank you M.

 
 Reply 
 

Product Spotlight

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window