Technical Discussions
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 233

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
233
09:37 Jun-26-2018
New edition of CSA W59 (2018) - changes to UT of welds

CSA has released the 2018 edition of W59 Welded Steel Construction, which includes major changes to the ultrasonic testing of structural welds. These include:

- selection of a variety of probe sizes and frequencies
- use of DAC/TCG for sensitivity calibration
- allowance for manual phased array

These are part of Annex X, which may be used instead of the classic fixed attenuation (FA) techniques in Clause 8.2.

 
 Reply 
 
THEO MICOTTIS
Italy, Joined May 2013, 82

THEO MICOTTIS

Italy,
Joined May 2013
82
09:55 Jun-26-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to Paul Holloway at 09:37 Jun-26-2018 (Opening).

Hi Paul,currently I don't have 2018 edition so I couldn't read it. Annex X can be used only be used with permission of engineer like previous annexes in older editions? Regards
Theo

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 233

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
233
13:04 Jun-26-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to THEO MICOTTIS at 09:55 Jun-26-2018 .

Hi Theo, great question.

I will make reference to the fixed attenuation technique in Clause 8.2 as the “FA technique”, and the new technique in Annex X as the “TCG technique”. That will save me from restating it multiple times below.

The TCG technique applies to manual conventional UT and manual PAUT and does not require engineering approval, but may be used "where agreed upon by the contractor and the welding inspection organization." Keep in mind this applies to *manual* UT/PAUT only, where probe oscillation and rastering is possible in order to maximize indication height. Encoded PAUT and other alternate techniques such as TOFD still require engineering approval as per Clause 8.2.12. Of course, in the long term we would all like encoded PAUT to be commonplace, but going all the way from an approach developed in 1969 to full-on encoded PAUT was inconceivably complex and would be impossible to achieve consensus on. As a result, we elected to develop a TCG approach and adopt manual PAUT as a first step.

I should point out that Annex X contains acceptance criteria modified to work with the TCG technique and provide quality levels consistent with the FA technique. So if you use Annex X, you use the new acceptance criteria. If you use the FA technique, then you keep doing things the way you were doing it before and use Tables 11.3 and 12.5. The acceptance levels in Annex X differ by a few dB from those in 11.3 and 12.5, which is due to the differences between actual attenuation and the linear estimation of 2 dB/inch. There is a white paper available on this published in the AWS Welding Journal in March 2018.

1
 
 Reply 
 
M G
,
Canada, Joined Nov 2017, 6

M G

,
Canada,
Joined Nov 2017
6
11:35 Jun-28-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to Paul Holloway at 09:37 Jun-26-2018 (Opening).

Hi, Paul

I haven't got the CSA W59 (2018), have few questions about the old version.
For the welds less than 8 mm, just tell the client we couldn't do it because there is not acceptance criteraia?

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 233

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
233
19:02 Jun-28-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to M G at 11:35 Jun-28-2018 .

You are correct.

 
 Reply 
 
M G
,
Canada, Joined Nov 2017, 6

M G

,
Canada,
Joined Nov 2017
6
07:41 Jul-01-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to Paul Holloway at 19:02 Jun-28-2018 .

Thanks

Sometimes we are requested to do SW on pipe welds with W59 because those pipe will be hit into ground as the base of top structure.
How can we scan the circ welds on 16"x 1/2" pipe(Might be smaller size) with the big monster probe as required by W59 , curve the wedge?

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 233

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
233
21:33 Jul-01-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to M G at 07:41 Jul-01-2018 .

I would hazard against using curved wedges with the FA technique as it will complicate the calibration. Besides, on a diameter as large as 16 inches I doubt it would amount to much difference.

Keep in mind that with the alternative in Annex X, you can now use much more appropriate search unit sizes and frequencies. Your application would be a great way to show your client the benefit of the recent changes.

 
 Reply 
 
Stan
NDT Inspector,
Canada, Joined Jan 2009, 31

Stan

NDT Inspector,
Canada,
Joined Jan 2009
31
15:52 Jul-02-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to Paul Holloway at 21:33 Jul-01-2018 .

Paul, thanks for this, it’s been a long time coming.
Do you know if the Code has been released yet, and when it comes into effect.
Regards
Stan

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 233

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
233
22:28 Jul-03-2018
Re: New edition of CSA W59 (2018) - changes to UT of welds
In Reply to Stan at 15:52 Jul-02-2018 .

Hi Stan:

It was released early June and is in effect now.

It is available on the CSA webstore, and will eventually make it's way into Techstreet and other sources.

Paul

 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>