Detection of inclusions in sheet steels by magnetic particle inspection.

Dear Sir/Madam,
I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.

Sincerely,
Kamran Azari


80, mousavi court
yahyakhan alley, chaharbagh bala ave.
Isfahan, 81736 67731
IRAN.


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
03:02 Aug-22-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
In rolled steel sheet Inclusions will be transformed by the rolling process into delaminations, parallel to the surface. MPI is unlikely to be an effective method to detect them, since in this orientation they will cause minimal disturbance to the flux lines. UT is likely to be a more effective method

Rgds

Joe

----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------




 
 Reply 
 
Sandro
Sandro
09:21 Aug-23-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------


Good morning Kamran Azari,
You have to know ASTM E-709 "Standard Guide for Magnetic Particle Examination"

Best regards,

Sandro
BOLIVIA




 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>