Detection of inclusions in sheet steels by magnetic particle inspection.

Dear Sir/Madam,
I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.

Sincerely,
Kamran Azari


80, mousavi court
yahyakhan alley, chaharbagh bala ave.
Isfahan, 81736 67731
IRAN.


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
03:02 Aug-22-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
In rolled steel sheet Inclusions will be transformed by the rolling process into delaminations, parallel to the surface. MPI is unlikely to be an effective method to detect them, since in this orientation they will cause minimal disturbance to the flux lines. UT is likely to be a more effective method

Rgds

Joe

----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------




 
 Reply 
 
Sandro
Sandro
09:21 Aug-23-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------


Good morning Kamran Azari,
You have to know ASTM E-709 "Standard Guide for Magnetic Particle Examination"

Best regards,

Sandro
BOLIVIA




 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window