kamran azari
03:39 Aug-22-2004
Detection of inclusions in sheet steels by magnetic particle inspection.

Dear Sir/Madam,
I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.

Sincerely,
Kamran Azari


80, mousavi court
yahyakhan alley, chaharbagh bala ave.
Isfahan, 81736 67731
IRAN.


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
03:02 Aug-22-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
In rolled steel sheet Inclusions will be transformed by the rolling process into delaminations, parallel to the surface. MPI is unlikely to be an effective method to detect them, since in this orientation they will cause minimal disturbance to the flux lines. UT is likely to be a more effective method

Rgds

Joe

----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------




 
 Reply 
 
Sandro
Sandro
09:21 Aug-23-2004
Re: Detection of inclusions in sheet steels by magnetic particle inspection.
----------- Start Original Message -----------
: Dear Sir/Madam,
: I am a M.Sc student in Materials science and technology. I,m very interested in the "detection of inclusions in cold rolled sheet steels by magnetic particle inspection". I need some information about the "current intensity and location (depth) and size of the inclusion which will be detected". Some articles have information about only two of them. Would you please send me some information relative to this subject.
: Sincerely,
: Kamran Azari
:
: 80, mousavi court
: yahyakhan alley, chaharbagh bala ave.
: Isfahan, 81736 67731
: IRAN.
------------ End Original Message ------------


Good morning Kamran Azari,
You have to know ASTM E-709 "Standard Guide for Magnetic Particle Examination"

Best regards,

Sandro
BOLIVIA




 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>