02:46 Aug-24-2004
I Need Help about "Inspection Plans for Welding Seams"

Hi! I am a post graduate student in Turkey. The subject of my thesis is "INSPECTION PLANS FOR WELDING SEAMS".

In my country i didnt find enough information about it. And i couldnt find enough information from the internet.

So if someone knows any internet address about this subject please send them to me.

Or if you have any more information, books, magazines, journals, .. something like that, please send them to me.

Regards,

Tugrul TURGUT

E-mail : tugrul_turgut@yahoo.com

Tel : +90 542 833 35 11

Address : Mimarsinan Cad. No:18/A Yalova/TURKEY


 
 Reply 
 
Mike Trinidad
Consultant,
LMATS Pty Ltd , Australia, Joined Jan 2003, 141

Mike Trinidad

Consultant,
LMATS Pty Ltd ,
Australia,
Joined Jan 2003
141
07:34 Aug-25-2004
Re: I Need Help about "Inspection Plans for Welding Seams"
G'Day Mr Turgut

I think you need to be a bit more specific in what you define as an "Inspection Plans for Welding Seams"

If you mean how to inspect welding seams you can use visual testing, penetrant testing, magnetic testing, electromagnetic testing, ultrasonic testing, acoustic emission testing, radiographic testing, leak testing, etc etc.

All the methods have different advantages and disadvantages and many of the methods have different methodologies e.g. ultrasonic testing ToFD, phased array.

Different methods and methodologies are used for different materials (steel, plastic) or different welding techniques (GTAW, FCW, FSW, GMAW, SAW, EGAW, SMAW, ESW etc, etc).

It's a balancing act between what defects you want to detect or specification, access, time constraints and probability of detection POD.


Regards

Mike

----------- Start Original Message -----------
: Hi! I am a post graduate student in Turkey. The subject of my thesis is "INSPECTION PLANS FOR WELDING SEAMS".
: In my country i didnt find enough information about it. And i couldnt find enough information from the internet.
: So if someone knows any internet address about this subject please send them to me.
: Or if you have any more information, books, magazines, journals, .. something like that, please send them to me.
: Regards,
: Tugrul TURGUT
: E-mail : tugrul_turgut@yahoo.com
: Tel : +90 542 833 35 11
: Address : Mimarsinan Cad. No:18/A Yalova/TURKEY
------------ End Original Message ------------




 
 Reply 
 
Tugrul TURGUT
Tugrul TURGUT
02:12 Aug-25-2004
Re: I Need Help about "Inspection Plans for Welding Seams"
Dear Mike,

I mean only inspection plans, not the inspection methods. For example, when you manufactured a steel bridge, a ship, a pressure vessel, etc etc,... you have to inspect it. And for the big constructions, you cant inspect all the welding seams.

Now, my question is which welding seams will we inspect and what the inspection order will be for welding seams? Which welding seam will we inspect first, and why?

Regards,
Tugrul TURGUT


----------- Start Original Message -----------
: G'Day Mr Turgut
: I think you need to be a bit more specific in what you define as an "Inspection Plans for Welding Seams"
: If you mean how to inspect welding seams you can use visual testing, penetrant testing, magnetic testing, electromagnetic testing, ultrasonic testing, acoustic emission testing, radiographic testing, leak testing, etc etc.
: All the methods have different advantages and disadvantages and many of the methods have different methodologies e.g. ultrasonic testing ToFD, phased array.
: Different methods and methodologies are used for different materials (steel, plastic) or different welding techniques (GTAW, FCW, FSW, GMAW, SAW, EGAW, SMAW, ESW etc, etc).
: It's a balancing act between what defects you want to detect or specification, access, time constraints and probability of detection POD.
:
: Regards
: Mike
: : Hi! I am a post graduate student in Turkey. The subject of my thesis is "INSPECTION PLANS FOR WELDING SEAMS".
: : I didnt find enough information about it. And i couldnt find enough information from the internet.
: : So if someone knows any internet address about this subject please send them to me.
: : Or if you have any more information, books, magazines, journals, .. something like that, please send them to me.
: : Regards,
: : Tugrul TURGUT
: : E-mail : tugrul_turgut@yahoo.com
: : Tel : +90 542 833 35 11
: : Address : Mimarsinan Cad. No:18/A Yalova/TURKEY
------------ End Original Message ------------




 
 Reply 
 
Ricardo
Ricardo
04:07 Aug-26-2004
Hi, saludos
saludos amigos pues me gustaria recibir links sobre la inspeccion visual de soldadura para aceros A36 (acero naval).

gracias
-----------------------------------------
i need links about inspection visual to Steel A36 (NAVAL STEEL)


 
 Reply 
 
Mike Trinidad
Consultant,
LMATS Pty Ltd , Australia, Joined Jan 2003, 141

Mike Trinidad

Consultant,
LMATS Pty Ltd ,
Australia,
Joined Jan 2003
141
04:47 Aug-26-2004
Re: I Need Help about "Inspection Plans for Welding Seams"
G'Day Mr Turgut

The decision whether or not to inspect something is based upon the risk of the component failing and the consequence of such a failure. This is also the definition for RBI (Risked Based Inspection) which is used to quantify the risk versus consequence in a matrix format. Before going to deep into RBI we should start back at the beginning.

In the beginning there wasn't many codes and if they did exist were basic. Companies at the time did what they felt was right based on experienced and some gambles. Storage tanks have an interesting history in this respect and in some ways still do as to the untrained eye they are a simple structure which cannot be easily mucked up. After several chatasrophic failures standards and specifications were drafted such as ASME and API to name just two. These standards specify almost everything including inspection amounts. So the most common way of determining the amount of NDT a component needs is by using a standard or specification that state the MINIMUM inspection requirements.

RBI goes, perhaps a step further with a full analysis of the process, contents, temperature, etc, etc to ensure components are being inspected that should be and components with low risk rankings are not.

If there is no standard for a component then an engineer with NDT experience or a NDT Level III can develop a procedure to inspect the component. This can be an easy task or a major research project dependent upon the component.

Something else I thought should be mentioned is the client or client representative often can request additional inspection or use the specifications to his advantage. For example API 650 for aboveground storage tanks specifies the number of radiographs which shall be taken on the welds which include horizontal seam welds, vertical seam welds and T joints. The client perhaps knows that the majority of the defects that occur will be in the T joints but the contractor will not radiograph them all unless the client pays more. Therefore the client decides that all the horizontal and vertical radiographs shall be done on the T joints. So to add another methodology for inspecting welds could be classified as experience based, wild card etc.

Hope that helps you out.

Regards

Mike

----------- Start Original Message -----------
: Dear Mike,
: I mean only inspection plans, not the inspection methods. For example, when you manufactured a steel bridge, a ship, a pressure vessel, etc etc,... you have to inspect it. And for the big constructions, you cant inspect all the welding seams.
: Now, my question is which welding seams will we inspect and what the inspection order will be for welding seams? Which welding seam will we inspect first, and why?
: Regards,
: Tugrul TURGUT
:
: : G'Day Mr Turgut
: : I think you need to be a bit more specific in what you define as an "Inspection Plans for Welding Seams"
: : If you mean how to inspect welding seams you can use visual testing, penetrant testing, magnetic testing, electromagnetic testing, ultrasonic testing, acoustic emission testing, radiographic testing, leak testing, etc etc.
: : All the methods have different advantages and disadvantages and many of the methods have different methodologies e.g. ultrasonic testing ToFD, phased array.
: : Different methods and methodologies are used for different materials (steel, plastic) or different welding techniques (GTAW, FCW, FSW, GMAW, SAW, EGAW, SMAW, ESW etc, etc).
: : It's a balancing act between what defects you want to detect or specification, access, time constraints and probability of detection POD.
: :
: : Regards
: : Mike
: : : Hi! I am a post graduate student in Turkey. The subject of my thesis is "INSPECTION PLANS FOR WELDING SEAMS".
: : : I didnt find enough information about it. And i couldnt find enough information from the internet.
: : : So if someone knows any internet address about this subject please send them to me.
: : : Or if you have any more information, books, magazines,journals, .. something like that, please send them to me.
: : : Regards,
: : : Tugrul TURGUT
: : : E-mail : tugrul_turgut@yahoo.com
: : : Tel : +90 542 833 35 11
: : : Address : Mimarsinan Cad. No:18/A Yalova/TURKEY
------------ End Original Message ------------




 
 Reply 
 
Ed T.
Ed T.
00:41 Aug-26-2004
Re: Hi, saludos
----------- Start Original Message -----------
: saludos amigos pues me gustaria recibir links sobre la inspeccion visual de soldadura para aceros A36 (acero naval).
: gracias
: -----------------------------------------
: i need links about inspection visual to Steel A36 (NAVAL STEEL)
------------ End Original Message ------------

www.onlinemetals.com/merchant.cfm?id=802&step=2
www.metalsdepot.com/products/ hrsteel2
www.techstreet.com/cgi-bin/detail?product_id=927951
www.ou.edu/class/hgruenwald/teach/4333/4333l11.htm


 
 Reply 
 
sandeep
sandeep
02:51 Aug-27-2004
regarding heat exchanger
hello friends , i am sandeep from india.i am a mechanical engineering engineering student. as a project , i am designing a heat exchanger with 3/8" tube OD, 2 passes, 1.25" traingular pitch , 13BWG, 6" shell dia. for these specifications how can i find the no. of tubes for different no of passes.what is the mathematical relation between no.of tubes and no. of tubes.
i would be very grateful to you..if u plz help me out.plz email me at.....
sandeepapawar@hotmail.com


 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window