ut test

Dear Sir,
I don’t know the criteria for selection of UT standards for quality assurance of welding from the design point of view. Indeed what is the difference between DIN 8563 and EN 25817 and when a designer should decide to check the welding in accordance to DIN 8563 or e.g. En 25817?
I will be grateful if you give me information about this matter.
With best regards,
Ali fasih



 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 183

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
183
01:10 Sep-06-2004
Re: ut test
reply:
Hello,

Please notice that DIN 8563 and also EN 25817 are obsolete.
These standards had to be withdrawn because now there are global standards for the quality of welded joints on metals:

1. EN ISO 5817 (December 2003)
Welding - Fusion welded joints in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections.

2. ISO/DIS 10042 (July 2004)
Welding - Arc-welded joints in aluminium and its weldable alloys - Quality levels for imperfections.

These global standards on weld quality are joined by an international standard on general rules for nondestructive testing of welds in metals:

3. ISO 17635 (September 2003)
Nondestructive testing of welds - General rules for fusion welds in metallic materials.

This standard is equivalent to EN 12062 (same title).

To link NDT to the designing of welds there is a new work item with CEN/Technical Committee 121:

4. WI 00121102
Welding - Design and nondestructive examination of welds.

In general:
All members of the European Union have to withdraw their national standards when a European (EN) or EN ISO standard is published on the same matter.
Before application of a national standard it is therefore necessary to check wether it is still valid and not superseeded by an international one.

Kind regards

Udo Schlengermann
Applications Laboratory
GE Inspection Technologies Systems GmbH
Huerth, Germany
Tel. +49-2233-601-550
Fax +49-2233-601-402
e-mail udo.schlengermann@ae.ge.com


----------- Start Original Message -----------
: Dear Sir,
: I don’t know the criteria for selection of UT standards for quality assurance of welding from the design point of view. Indeed what is the difference between DIN 8563 and EN 25817 and when a designer should decide to check the welding in accordance to DIN 8563 or e.g. En 25817?
: I will be grateful if you give me information about this matter.
: With best regards,
: Ali fasih
------------ End Original Message ------------





 
 Reply 
 
sudher
sudher
02:17 Sep-07-2005
Re: ut test
surveyor told me to do ultrasonic test as per german standard for structural joints(ship building)..what acceptance criteria should i use if it for weld


 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window