Hi guys

I have a question

For UT shear wave weld inspection of butt weld on 2'' diameter piping, i can use basic calibration block given in ASME ,Figure T-434.3-2 for DAC curve, right? i will use the same material specification group P1.
Later, do a i need the dac offset curve al 6db and 12db for rejection criteria? or with the principal curve dac is enough?

thanks

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 227

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
227
22:21 Apr-06-2019
Re: DAC calibration using curved Block
In Reply to Rene at 01:05 Apr-06-2019 (Opening).

Hi Rene:

Yes, absolutely you can use the alternative block shown in Fig. T-434.3-2. You will need to generate a DAC/TCG, and then add 6dB of scanning gain as per T-471.4.1.

The rejection level (re: your 6dB or 12dB offset from reference) will depend on the code that you are inspecting to. If they are ASME B31.3 (process piping) welds, then the rejection level is actually the reference level (i.e. unless the indication breaks DAC, ignore it).

1
 
 Reply 
 
Rene
El Salvador, Joined Apr 2019, 3

Rene

El Salvador,
Joined Apr 2019
3
03:48 Apr-07-2019
Re: DAC calibration using curved Block
In Reply to Paul Holloway at 22:21 Apr-06-2019 .

Thanks Paul,

I will examine a 1/4" thick overheating pipe, can i generate the DAC curve only with a 1mm side drill hole at half the thickness as reference level?

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 227

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
227
10:39 Apr-07-2019
Re: DAC calibration using curved Block
In Reply to Rene at 03:48 Apr-07-2019 .

Unfortunately you won't be able to use a SDH. ASME states that the hole must be 38mm (1.5“) long and you simply won't be able to drill that on a 2" OD and 1/4" thick pipe. There's not enough material.

 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window