probe size in paut

can any one share the idea to select probe size for weld inspection depending on the thickness?

    
 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 701

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
701
16:37 May-14-2019
Re: probe size in paut
In Reply to saroj at 09:00 May-12-2019 (Opening).

Use larger aperture with increase in thickness.
What thickness are you inspecting ?

    
 
 
Andrej
ApplusRtd, Lithuania, Joined May 2019, 6

Andrej

ApplusRtd,
Lithuania,
Joined May 2019
6
20:11 May-14-2019
Re: probe size in paut
In Reply to saroj at 09:00 May-12-2019 (Opening).

Do you have any procedure?

    
 
 
NOUFEL.T.MUHAMMED
NOUFEL.T.MUHAMMED
19:13 May-15-2019
Re: probe size in paut
In Reply to saroj at 09:00 May-12-2019 (Opening).

You can use the parameter 'PITCH' for probe selection for thickness variations.
Lower thickness(<7mm)-use 0.3mm pitch probes
medium thickness(7mm-50mm)-use 0.6mm pitch probes
Higher thickness (>50mm)-use 1mm pitch probes
*contents as per my experience only.

    
 
 

Product Spotlight

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window