13:09 Jul-12-2019
dpt possibility

sir

here is a querry from one of my friends in railways. he asked me whether DPT is possible over head position? i say YES
he is using method-c, type ii form d penetrant testing (solvent removable penetrant, visible , non aqueious suspended developer.

is any standard related to DPT over head position
testing of weld under rail bogie

plz justify my answer

    
 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 740

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
740
14:11 Jul-12-2019
Re: dpt possibility
In Reply to bommakanti srinivas at 13:09 Jul-12-2019 (Opening).

No issue, he is good to go

    
 
 Reply 
 
Gerald Reams
Engineering,
Industry, USA, Joined Aug 2012, 180

Gerald Reams

Engineering,
Industry,
USA,
Joined Aug 2012
180
14:31 Jul-12-2019
Re: dpt possibility
In Reply to bommakanti srinivas at 13:09 Jul-12-2019 (Opening).

DPT works by capillary action, not by gravity. The position of the test does not matter.

Gerald Reams

    
 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

CIVA 2017 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window