1115 views
Technical Discussions
John G.
John G.
04:02 Oct-05-2004
IQI Rrequirements

What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
What material would your IQI be made of and what thickness would you base it on?


 
 Reply 
 
Buddy
Buddy
04:29 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

You IQI selection would be the same for either material. ASME SE-1025, referenced in ASME V, Article 2, groups carbon and stainless steels in the same material group (Group 1) and requires the IQI to be manufactured from either carbon steel or 300 series stainless.



 
 Reply 
 
Buddy
Buddy
04:35 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.


 
 Reply 
 
Anonymous
Anonymous
01:03 Oct-06-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : What material would your IQI be made of and what thickness would you base it on?
: Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
------------ End Original Message ------------

So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?



 
 Reply 
 
Buddy
Buddy
02:52 Oct-07-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : : What material would your IQI be made of and what thickness would you base it on?
: : Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
: So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?
------------ End Original Message ------------
Good point. I believe that since clad is added after the weld is completed, the weld and reinforcement should be examined by RT first, using the appropriate IQI. After the clad is added, that would be examined by PT. I believe this is as stated in ASME III NB-5272. Can't say for other codes.




 
 Reply 
 

Product Spotlight

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>