21:00 Aug-07-2019
PCN AND ISO

Dear experts,


What is the difference between BS EN ISO9712:2012 and EN 473?

Can we use ISO9712 LEVEL II Wherever pcn was asked by recruiter?

    
 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 177

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
177
10:14 Aug-08-2019
Re: PCN AND ISO
In Reply to Seenikumaran at 21:00 Aug-07-2019 (Opening).

Seenikumaran,
to answer your questions:
- In 2010 the process was started to replace EN 473:2008 by a revised version of ISO 9712:2005 as a combined EN ISO standard.
This the actual version now (EN ISO 9712 is identical to ISO 9712):
ISO 9712:2012, Non-destructive testing - Qualification and certification of NDT personnel.
By this date the European Standard EN 473 has been withdrawn.

- ISO 9712 is an International Standard only, whereas PCN is a certification scheme run by the BINDT.
More national certification schemes are based on ISO 9712.

With best regards

    
 
 Reply 
 

Product Spotlight

FlexoFORM™

The FlexoFORM™ solution integrates flexible phased array probe technology in a scanner to solv
...
e the challenges that come with inspecting pipe elbows. When combined with a water column, this solution can be used to collect easy-to-interpret data on elbows with diameters ranging from 4.5 in. OD up to flat and offers many benefits.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

CIVA 2017 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window