17:24 Aug-14-2019
velocity of different steels

I am not having much luck in my research. does anyone have any input on the velocity of different steels. i work in the bridge industry and use alot of A709 or M270. my question is in regards to the different grades 50, 50w, 70w, 70hps. are the velocities different for all of these?if so is it a big enough difference to effect my sensitivity and angle calibration for UT? any input is welcomed. i currently use the type2 iiw block for cal.

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 808

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
808
20:40 Aug-17-2019
Re: velocity of different steels
In Reply to Steve Amspacher at 17:24 Aug-14-2019 (Opening).

All carbon steels have practically the same velocity. Austenitic stainless is slightly different

 
 Reply 
 
Ali
NDT Inspector,
Iran, Joined Mar 2013, 117

Ali

NDT Inspector,
Iran,
Joined Mar 2013
117
13:07 Aug-18-2019
Re: velocity of different steels
In Reply to Steve Amspacher at 17:24 Aug-14-2019 (Opening).

It depends on material fabrication process.if the material is anisotropic it will change velocity and angle of beams.this happen usually in large diameter pipes in pipline , for example pipe is 5LX65 and carbon steel, because of production process and heat treatment,material grains will be anisotropic and velocity of shear wave will be around 3.350 up to 3.4 mm per micro second instead of 3.230.
also if the same material change to seamless (specially thick pipes and small diameter ) cause of different production process it would be coarse grain and very attenutive. It is better to prepare calibration block from the material that we are going to inspect.if you dont have access to the material, you can perform transfer correction on both cal block and production weld base metals to get similar velocity and sensitivity.
Also check below article from Mr Ed Ginzel.

https://www.ndt.net/search/docs.php3?id=21545

 
 Reply 
 
Ali
NDT Inspector,
Iran, Joined Mar 2013, 117

Ali

NDT Inspector,
Iran,
Joined Mar 2013
117
13:18 Aug-18-2019
Re: velocity of different steels
In Reply to Ali at 13:07 Aug-18-2019 .

This link is correct.
https://www.ndt.net/search/docs.php3?id=19091

1
 
 Reply 
 

Product Spotlight

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window