IQI Rrequirements

What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
What material would your IQI be made of and what thickness would you base it on?


 
 Reply 
 
Buddy
Buddy
04:29 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

You IQI selection would be the same for either material. ASME SE-1025, referenced in ASME V, Article 2, groups carbon and stainless steels in the same material group (Group 1) and requires the IQI to be manufactured from either carbon steel or 300 series stainless.



 
 Reply 
 
Buddy
Buddy
04:35 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.


 
 Reply 
 
Anonymous
Anonymous
01:03 Oct-06-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : What material would your IQI be made of and what thickness would you base it on?
: Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
------------ End Original Message ------------

So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?



 
 Reply 
 
Buddy
Buddy
02:52 Oct-07-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : : What material would your IQI be made of and what thickness would you base it on?
: : Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
: So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?
------------ End Original Message ------------
Good point. I believe that since clad is added after the weld is completed, the weld and reinforcement should be examined by RT first, using the appropriate IQI. After the clad is added, that would be examined by PT. I believe this is as stated in ASME III NB-5272. Can't say for other codes.




 
 Reply 
 

Product Spotlight

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window