IQI Rrequirements

What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
What material would your IQI be made of and what thickness would you base it on?


 
 Reply 
 
Buddy
Buddy
04:29 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

You IQI selection would be the same for either material. ASME SE-1025, referenced in ASME V, Article 2, groups carbon and stainless steels in the same material group (Group 1) and requires the IQI to be manufactured from either carbon steel or 300 series stainless.



 
 Reply 
 
Buddy
Buddy
04:35 Oct-05-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: What material would your IQI be made of and what thickness would you base it on?
------------ End Original Message ------------

Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.


 
 Reply 
 
Anonymous
Anonymous
01:03 Oct-06-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : What material would your IQI be made of and what thickness would you base it on?
: Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
------------ End Original Message ------------

So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?



 
 Reply 
 
Buddy
Buddy
02:52 Oct-07-2004
Re: IQI Rrequirements
----------- Start Original Message -----------
: : : What would the IQI requirements be for carbon steel pipe with Stainlness steel cladding?
: : : What material would your IQI be made of and what thickness would you base it on?
: : Sorry-base you IQI selection on the material thickness under examination, including any weld reinforcement allowed by the referencing code section. The above two answers are based on you using the ASME code. For others (AWS/API etc.) use the code requirements. IF your code referes you to ASME V, then the above applies. Good luck.
: So if you are shooting a 1" thick c/s pipe with 1/8" thick s/s cladding on the ID, you would base your IQI on 1" of c/s and not the cladding? Is that correct?
------------ End Original Message ------------
Good point. I believe that since clad is added after the weld is completed, the weld and reinforcement should be examined by RT first, using the appropriate IQI. After the clad is added, that would be examined by PT. I believe this is as stated in ASME III NB-5272. Can't say for other codes.




 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>