Black light integrity check Interval(ASTM E1444)

I would like to ask about the black light integrity check Interval According to E1444M (REV−16), different phrases for integrity can be identified.

Weekly checks are specified in TABLE 1 Required Verification Intervals.
However, Section 7.3.2 says to check every day.

Why is this difference?

Is there a checklist and procedure for black light integrity?
Looking forward to your response, thank you first.


ASTM E1444
7.3.2 Black Lights—Black lights used for evaluation purposesshall meet the requirements of 7.4.5. The minimumacceptable intensity is 1000 μW / cm2 at the surface beingexamined. Black lights shall be checked daily for cleanlinessand integrity and shall be cleaned, repaired or replaced asappropriate.

 
 Reply 
 
Rick Lopez
R & D,
John Deere - Moline Technology Innovation Center, USA, Joined Jul 2011, 191

Rick Lopez

R & D,
John Deere - Moline Technology Innovation Center,
USA,
Joined Jul 2011
191
15:04 Aug-23-2019
Re: Black light integrity check Interval(ASTM E1444)
In Reply to JOONGHWAN at 07:56 Aug-21-2019 (Opening).

Hello Joonghwan,
I am not aware of a specific checklist, but I believe that the words following "integrity" indicate what is of interest here: condition (e.g. cracked/chipped/missing) of the UV-A radiation path (e.g. filter, splash guard) and radiation source (black light) itself.
Regards

 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window