ASTM 2175 Requirements of penetrant inspection

Hi,
Did someone work with this standard in refer to PT.
I need information about what is subject of evaluation discontinuities or indications??
Thank in advance.

 
 Reply 
 
SUMURAY
SUMURAY
18:45 Aug-21-2019
Re: ASTM 2175 Requirements of penetrant inspection
In Reply to Grzegorz at 11:52 Aug-21-2019 (Opening).

Excuse me SIR.
are you sure of this standard is correct?
I Think is ASTM E1417 or ASTM E165.

 
 Reply 
 
Grzegorz
NDT Inspector,
Poland, Joined Feb 2012, 15

Grzegorz

NDT Inspector,
Poland,
Joined Feb 2012
15
08:00 Aug-22-2019
Re: ASTM 2175 Requirements of penetrant inspection
In Reply to SUMURAY at 18:45 Aug-21-2019 .

Sie,
You're right, these mentioned by you standards refer to PT, but both contain only parameters for carring out of test.
ASTM 2175 contains only requirements of all NDT tests among others PT.

 
 Reply 
 

Product Spotlight

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window