Lead Marker for RT

Hi guys,

i have a question whether there are other options other than lead marker for RT works..

i am wondering whether there is a type of pen(i literally mean pen) that contain lead inks/filler to replace the conventional lead markers that are widely used in this industry.

thanks in advance guys. cheers..

 
 Reply 
 
SF
SF
08:38 Aug-22-2019
Re: Lead Marker for RT
In Reply to Nafis at 15:09 Aug-21-2019 (Opening).

SFD

 
 Reply 
 
Matthias
NDT Inspector, CEO
Dreifeld Materialprüftechnik, Germany, Joined Sep 2005, 105

Matthias

NDT Inspector, CEO
Dreifeld Materialprüftechnik,
Germany,
Joined Sep 2005
105
10:40 Aug-22-2019
Re: Lead Marker for RT
In Reply to Nafis at 15:09 Aug-21-2019 (Opening).

I don't think so since its toxic.

 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
09:24 Aug-26-2019
Re: Lead Marker for RT
In Reply to Nafis at 15:09 Aug-21-2019 (Opening).

Hi,
I have seen radiographers use a typed or printed ID info on a transparent sheet, and the film when exposed to radiation has a small area (same size as the ID) covered with lead. After exposure to radiation, the film cassette was opened in the dark room and then the ID sheet was placed on the unexposed area and just that small ID bit exposed to light in a device.
This then transferred to ID info onto the film.

You have to be careful not to mix films up, but it is an alternative to using lead for ID.
You still need to use lead markers when testing larger areas with multiple shots (such as welds)


Godfrey

 
 Reply 
 

Product Spotlight

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>