where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

IMG ULTRASUONI SRL
Ultrasonic transducers for industrial applications (NDT) and medical (Doppler effect). Probes, Ultrasonic instruments, Special systems for NDT.
611 views
Technical Discussions
bounatiro
Algeria, Joined Aug 2019, 3

bounatiro

Algeria,
Joined Aug 2019
3
19:22 Aug-22-2019
radiography piping fill with water

dear expert
Our, company is contacted to do radiography for the welding joint of thin joint of piping diameter from 2 to 20", but the problem is almost the piping is filled with water, I searched any standard for doing radiography but unfortunately I didn't find any way,
please share your experience

 
 Reply 
 
laurie
Australia, Joined Feb 2019, 37

laurie

Australia,
Joined Feb 2019
37
02:56 Aug-23-2019
Re: radiography piping fill with water
In Reply to bounatiro at 19:22 Aug-22-2019 (Opening).

There aren't any standards that I know of for this situation but you can radiograph the joint.
Work out the equivalent thickness of steel for your water path, and then work out your achievable sensitivity and see if it meets code requirements.
HVL for water with IR192 is something like 70mm.
So your 2" with water would be equivalent to about an extra 10 mm of steel and the 20" about an extra 100 mm of steel.
Sensitivity might be ok for the 2" but 20" is no chance.
You would need to do test exposures to confirm sensitivity and you'd probably need 8 exposures to narrow your diagnostic length to improve the sensitivity for that region.

 
 Reply 
 
Shane Feder
, Quality Co-ordinator (SubSea)
Thailand, Joined Dec 2014, 89

Shane Feder

, Quality Co-ordinator (SubSea)
Thailand,
Joined Dec 2014
89
15:02 Aug-27-2019
Re: radiography piping fill with water
In Reply to laurie at 02:56 Aug-23-2019 .

Laurie has given you good advise.
It is very, very hard to get a code compliant radiograph with the pipe filled with water.
If you can meet sensitivity and density requirements then you can interpret but you will need test shots on all diameters and thicknesses first.

 
 Reply 
 
Angel
Angel
19:44 Sep-01-2019
Re: radiography piping fill with water
In Reply to laurie at 02:56 Aug-23-2019 .

2" pipe diameter- equivalent 10mm?
I made pipe with and without water with 4mm thickness and diameter 30mm - the same set up - density and sensitivity were similar, sensitivity hard to note

 
 Reply 
 
bounatiro hatem
Algeria, Joined Aug 2019, 3

bounatiro hatem

Algeria,
Joined Aug 2019
3
20:08 Sep-02-2019
Re: radiography piping fill with water
In Reply to Angel at 19:44 Sep-01-2019 .

Dear Expert

Thanks for all answer, us you said, i agree with my client to do some sample according to the idea of laurie, when i will do it i will share with you my radiogramme


Many thanks

 
 Reply 
 

Product Spotlight

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window