Finding Debonding between composites

Hello All,

Could anyone help me out with below mentioned two different cases

Case I- Sandwich structure made of Carbon Steel (CS-5 mm) + Polyurethane (PU-10 mm) + Carbon Fibre (CF-10mm). is there any practical solution to find debonding(planner or volumetric) between Interface 1(CS-PU) and Interface 2 (PU-CF).
Access for UT from only one side (Carbon steel side)

Case II- Sandwich structure made of CF (15 mm)+ PU(15mm) + CF (10 mm).
Same finding as Case I.
Access from only one side.

 
 Reply 
 
Wiesław Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 271

Wiesław Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
271
10:37 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Immersion or contact testing should be possible in the first case, but it will be necessary to use transducer with quite short pulse and quite sophisticated signal analysis, since the difference between total reflection and transmission into plastic is not very strong and many internal reflexions in steel can be expected.
Second case is more difficult due to the fact, that CF and PU are not very different and CF is quite attenuating. It should work, but requires careful development of suitable procedures.

2
 
 Reply 
 
Anand
India, Joined Jul 2016, 1

Anand

India,
Joined Jul 2016
1
10:40 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Hi,
Myself Anand.

I think UT will work for composites.Based on my work experience I'm telling. But the combination of metal and composites, I am not sure.

Thanks.

1
 
 Reply 
 
Daniel Braun
Daniel Braun
12:49 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Generally it is possible, if you have the samples available - you may ship them to Sonotron NDT A-Lab for performing the trials and laying out the necessary setup (instrument, probe, settings) - if you're interesting simply e-mail and we'll proceed further. The service is FOC

 
 Reply 
 
Andres Romero
NDT Inspector,
Spain, Joined Jul 2019, 9

Andres Romero

NDT Inspector,
Spain,
Joined Jul 2019
9
04:26 Aug-24-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

zoom image



Hello, sorry for my English is not good.
If possible, by immersion. With squirt machine.
Several frequencies are needed.
 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window