where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

ZETEC, Inc.
Zetec is a global leader in nondestructive testing (NDT) solutions for the critical inspection needs of industries the world counts on every day, ...
560 views
Technical Discussions
Nikos Roussos
Greece, Joined Aug 2019, 2

Nikos Roussos

Greece,
Joined Aug 2019
2
21:33 Sep-01-2019
PAUT inspection of thick welds
zoom image

weld

Dear experts,
I‘ve been asked if I can inspect properly welded pipes with thickness of 90mm.
The equipment that I have is a Sonatest Prisma 16:64 with X3-PE-5.0M64E0.6P 64 element probe. I will also use a weld scanner from Phoenix.
Do you think my equipment is capable of giving me reliable results in such thick welds with the geometry shown in the figure? Do you think I should get a sensor with less frequency (2,25 or 3,5 MHz)?
Additional to PAUT inspection I will also perform TOFD, but my main concerns are for the PAUT.

 
 Reply 
 
Creed
NDT Inspector,
n.n., Joined Jul 2009, 33

Creed

NDT Inspector,
n.n.,
Joined Jul 2009
33
06:15 Sep-02-2019
Re: PAUT inspection of thick welds
In Reply to Nikos Roussos at 21:33 Sep-01-2019 (Opening).

First of all, the inspection should be performed following the standard and acceptance criteria or your company procedure writing; follow the standard, I am pretty sure you will have the answer YES or NO for your question.
My opinion you need to conduct the inspection with multi scans to cover entire the weld body, however based on the sketch of weld configuration the bevel angle should be concerned as a limitation, due to oriental of the fusion face defects wouldn't give the good refection with the PAUT sectorial beam.

1
 
 Reply 
 
Elias Campanario
Engineering,
Tecnicas Reunidas, Spain, Joined Oct 2013, 3

Elias Campanario

Engineering,
Tecnicas Reunidas,
Spain,
Joined Oct 2013
3
10:22 Sep-02-2019
Re: PAUT inspection of thick welds
In Reply to Nikos Roussos at 21:33 Sep-01-2019 (Opening).

Dear Nikos;

Regarding your question, in my opinion, the best solution in your case would be to combine inspection by ToFD and PAUT.

In any case, you should make a mock up with notches in the welding bevel, in which to test the scan plan that you generate for the inspection.

As for the PAUT probes, maybe for that thickness you need a 3.5 or 2.25 MHz probe.
With the 5MHz probe, maybe you to have a lot of noise at great depth.

I hope I've helped.

1
 
 Reply 
 
Ali
NDT Inspector,
Iran, Joined Mar 2013, 105

Ali

NDT Inspector,
Iran,
Joined Mar 2013
105
15:39 Sep-02-2019
Re: PAUT inspection of thick welds
In Reply to Nikos Roussos at 21:33 Sep-01-2019 (Opening).

this bevel configuration is not suitable for PAUT Sectorial scan but you can apply Tofd for better detection of side wall defect.If you have access to inside of vessel,perform Tofd and PAUT scan from out side and inside ( only half skip for PAUT) .this technique will reduce tofd dead zone only in backwall area and for PAUT will reduce sound path and increase signal to nois ratio in half skip instead of full skip scan.
Hope material grains is fine and surface is not wrought for PAUT and Tofd inspection.

1
 
 Reply 
 
laurie
Australia, Joined Feb 2019, 34

laurie

Australia,
Joined Feb 2019
34
02:35 Sep-03-2019
Re: PAUT inspection of thick welds
In Reply to Nikos Roussos at 21:33 Sep-01-2019 (Opening).

If you're going to be doing more of this type of work I'd suggest your boss might have to stump up for some simulation software.

Use a simulator like UTMan which from memory is something like 100 Euro and does manual UT, TOFD and AUT.
http://www.utsim.co.uk/index.html

If you have a couple of thousand dollars then Beamtools will do everything and also has sectorial beamset beam energy display which would be a big help for your long beam paths.
https://www.eclipsescientific.com/beamtool.html

There are lots of others including Olympus NDT SetupBuilder
https://www.olympus-ims.com/en/omniscan-software/#!cms[tab]=%2Fomniscan-software%2Fndt-setupbuilder

 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window