bond tester - signal evaluation

We are working with ZETEC Bond Tester S21R in sondicator mode for honeycomb structure test. We are able to record 1inch D disbond, but indication from that decrease to 1/2 of origin using 12 dB. It is OK ? According to general formula 20log H1/H2 should be 6 dB. Do you have anybody explanation ? Thank you.

 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
11:55 Jul-24-2009
Re: bond tester - signal evaluation
In Reply to Jiri Brus at 10:02 Jul-24-2009 (Opening).

The Gain steps on The Zetec MIZ-21 series are 1/2 dB, Not 1 dB so a gain change of 12 is 6dB

This is explained in the manual, (Section 4.5.8 Probe Gain, page 4-13 in the MIZ-21 Manual, I don't have the S21R version immediately to hand) but who reads them that closely...

I have to say it confused me at first, and on a bad day it still does...

Joe

 
 Reply 
 
joel nyaga
joel nyaga
10:41 Sep-07-2019
Re: bond tester - signal evaluation
In Reply to Joe Buckley at 11:55 Jul-24-2009 .

Who could be having a zetec bond tester S-21R version to send to me. am having problems trying to use x-y mode (flying dot disbond measurement) and delamination setups.

 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window