305 views
Technical Discussions
Veera
Veera
06:43 Nov-27-2019
Radiography Testing of Fluid filled Piping.

Dear Experts,
We have issue in RT,Client asking to perform RT in Fluid Filled Lines(Like Gasoline,Diesel..Etc),is it possible to get the accurate results,and any procedure required for those job,plz suggest.

 
 Reply 
 
Carlos A. Galán
NDT Inspector,
UIS - Universidad Industrial de Santander, Colombia, Joined Oct 2014, 33

Carlos A. Galán

NDT Inspector,
UIS - Universidad Industrial de Santander,
Colombia,
Joined Oct 2014
33
03:52 Nov-28-2019
Re: Radiography Testing of Fluid filled Piping.
In Reply to Veera at 06:43 Nov-27-2019 (Opening).

hello Veera

If it is possible to obtain precise results considering the corrections in exposure conditions due to the density and distance that x-rays pass through (energy absorption is low).

If the fluid has particles of considerable size, or has considerable internal dirtiness could cause low quality in the film.


Bye

 
 Reply 
 
Dr. Uwe Zscherpel
Director,
BAM Berlin, Germany, Joined Jan 2010, 89

Dr. Uwe Zscherpel

Director,
BAM Berlin,
Germany,
Joined Jan 2010
89
08:46 Dec-02-2019
Re: Radiography Testing of Fluid filled Piping.
In Reply to Carlos A. Galán at 03:52 Nov-28-2019 .

Dear Veera,

in principle it is easily possible to inspect pipes filled with media by RT. The limitations depend on the pipe material and dimensions as well as the media. Please see for procedures ISO 20769 from 2018: "NDT - Radiographic inspection of corrosion and deposits in pipes by X- and gamma-rays, Part 1: tangential radiographic inspection, Part 2: double wall radiographic inspection"

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window