UT & RT inspection of butt fusion welds in PVC pipe

We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.

Regards,

Fred Raco, Jr.


 
 Reply 
 
Mike Troughton
Mike Troughton
05:15 Mar-01-2004
Re: UT & RT inspection of butt fusion welds in PVC pipe
We have been carrying out research into UT and RT inspection of butt fusion welds in PE pipes for around 15 years and have published many papers on the subject, e.g.

Troughton M J: "Welding with integrated non-destructive examination of polyethylene pipes". Plastics Pipes XI Conference, Munich, Germany, 3-6 September 2001.

Munns I J and Georgiou G A: "Ultrasonic and radiographic NDT of butt fusion welded polyethylene pipes", Insight 41(5), 291.

We are also currently developing new NDT techniques for both butt fusion and electrofusion welds in PE pipes.

PVC pipes are rarely butt fusion welded. They are normally joined using a solvent cement. However, if you are indeed looking to carry out NDT on PVC butt fusion welds, then these papers would be a good starting point.

----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------




 
 Reply 
 
ams_ati
ams_ati
08:05 Nov-21-2004
Re: UT RT inspection of butt fusion welds in PVC pipe
i need some information about ndt ( specialy new ndt methods ) in inspection of electrofusion welds in PVC pipe. i'm student of mechanical engineering.
thanks----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------





 
 Reply 
 
M. Biglar
M. Biglar
06:35 Feb-06-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------

I am a student at mechanical Eng. and start a project about pe pipe joint inspection with N D T method please guide me about this method.
Thanks for your attention



 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 182

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
182
06:54 Feb-09-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
as in Feb 2005 the request for UT of welds in PVC pipe appeared again in this forum, a useful information for all readers:

Active from November 2004 there is a new European Standard:
EN 13100-3
Nondestructive testing of welded joints in thermoplastics semi-finished products -
Part 3: Ultrasonic testing

Kind regards
Udo Schlengermann
GE Inspection Technologies GmbH
Huerth, Germany

----------- Start Original Message -----------
: : We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: : Regards,
: : Fred Raco, Jr.
: I am a student at mechanical Eng. and start a project about pe pipe joint inspection with N D T method please guide me about this method.
: Thanks for your attention
------------ End Original Message ------------





 
 Reply 
 
marjan
marjan
07:55 Sep-17-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
------ Dear sirs
We are a group of employees of National iranian Gas
company(N.IG.C).Polyethylene pipes are used in the gas distribution system
of Iran and we are seeking to provide coupler for electrofusion joints.Our
main problem is joint inspection.Please kindly let us know the answer of the
following questions:

1-what are the inspection methods for electrofusion joints and which
one is preferred?

2-Does NDT "non destructive test"method exist for joint inspection
and if so,what are the equipments and standards and expenses.

3-Does NDT method provide inspection and confirmation the quality
lonely or the DT and NDT should be carried out simultaneously.


Sincerely yours

M.yousefi

----- Start Original Message -----------
: We have been carrying out research into UT and RT inspection of butt fusion welds in PE pipes for around 15 years and have published many papers on thesubject, e.g.
: Troughton M J: "Welding with integrated non-destructive examination of polyethylene pipes". Plastics Pipes XI Conference, Munich, Germany, 3-6 September 2001.
: Munns I J and Georgiou G A: "Ultrasonic and radiographic NDT of butt fusion welded polyethylene pipes", Insight 41(5), 291.
: We are also currently developing new NDT techniques for both butt fusion and electrofusion welds in PE pipes.
: PVC pipes are rarely butt fusion welded. They are normally joined using a solvent cement. However, if you are indeed looking to carry out NDT on PVC butt fusion welds, then these papers would be a good starting point.
: : We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: : Regards,
: : Fred Raco, Jr.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window