where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

EKOSCAN
EKOSCAN is a French manufacturer specialized in equipment for ultrasonic Non Destructive Testing: Probes,UT boards & Scanners tailored for your needs
428 views
Technical Discussions
Dhiae
ISQ, Algeria, Joined Jan 2020, 4

Dhiae

ISQ,
Algeria,
Joined Jan 2020
4
14:57 Jan-16-2020
PAUT ( corrosion mapping) high temperature Solution.

Hi inspectors,
that's my first subject on ndt.net, i have an issues on application of corrosion mapping in high temperature (73 °C) using Omniscan X2 ( SA12 Probe), what im doing now is to change the coupling after two indication, and its helpful, but i dont want to risk the equipment ( probe ), is there any solution for that problem?

 
 Reply 
 
Creed
NDT Inspector,
Vietnam, Joined Jul 2009, 34

Creed

NDT Inspector,
Vietnam,
Joined Jul 2009
34
04:59 Jan-17-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Dhiae at 14:57 Jan-16-2020 (Opening).

Can you use HydroForm probe for corrosion mapping?

 
 Reply 
 
Dhiae
ISQ, Algeria, Joined Jan 2020, 4

Dhiae

ISQ,
Algeria,
Joined Jan 2020
4
06:45 Jan-17-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Creed at 04:59 Jan-17-2020 .

No, i cant because the surface it not hellping.

 
 Reply 
 
laurie
Australia, Joined Feb 2019, 36

laurie

Australia,
Joined Feb 2019
36
14:24 Jan-18-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Dhiae at 14:57 Jan-16-2020 (Opening).

HydroForm might be your solution.
The water delay and constant water feed would keep the heat away from the probe and the water path would give you good results.

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 227

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
227
19:27 Jan-18-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to laurie at 14:24 Jan-18-2020 .

Good idea Laurie. Also, the 73 deg C might cause the adhesive on the HydroFORM gaskets to wear out quicker. That's pretty warm but not ridiculous. I'd say just make sure the bag of gaskets is full before the job starts. And setup all the spare parts so they can do quick changes in the field and keep running.

HydroFORM is a great product.

 
 Reply 
 
Dhiae
ISQ, Algeria, Joined Jan 2020, 4

Dhiae

ISQ,
Algeria,
Joined Jan 2020
4
07:00 Jan-19-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Paul Holloway at 19:27 Jan-18-2020 .

Paul,

about the rough surface ( external corrosion ) we clean the pipe before inspection with bronze hammer and metallic brash, i make the surface clean and i do the inspection,
and about the hydro-form, its not helping, because the surface its very corroded and that make it so hard for the gaskets to stay in shape.

 
 Reply 
 
laurie
Australia, Joined Feb 2019, 36

laurie

Australia,
Joined Feb 2019
36
08:58 Jan-19-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Dhiae at 07:00 Jan-19-2020 .

If the surface is very corroded the RexoForm has a 20mm Rexolite delay wedge and it looks like you can order with water feed nozzles.

 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 227

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
227
20:06 Jan-19-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Dhiae at 07:00 Jan-19-2020 .

External corrosion? In that case, get out your grid sheets and your pen probe. You could mess around all day and night fighting with a PAUT setup and get nowhere... or you could just do it old school and get it over with.

 
 Reply 
 
laurie
Australia, Joined Feb 2019, 36

laurie

Australia,
Joined Feb 2019
36
21:47 Jan-19-2020
Re: PAUT ( corrosion mapping) high temperature Solution.
In Reply to Paul Holloway at 20:06 Jan-19-2020 .

Depending on how bad the surface is UT might only be part of the solution.
A straight edge and pit gauge with spot or grid measurements where you can is often the best solution.
RollerForm, HydroForm, RexoForm, small diameter twin or single crystal probes including pen probes, pit gauges and straight edges all have their place but alone none of them will cover every situation.

 
 Reply 
 

Product Spotlight

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window