ASME RAD Ref. Code Penetreted Thickness.

With regards ASME V article 2, estimated penetrated thickness (WT+excess metal), shall not exceed the maximum stated by the referencing code.

Could anyone advise which sections of ASME B31.3, VII and IX, that this information can be found.

 
 Reply 
 
Diego
Consultant,
Freelance, Spain, Joined May 2013, 197

Diego

Consultant,
Freelance,
Spain,
Joined May 2013
197
12:26 Mar-25-2020
Re: ASME RAD Ref. Code Penetreted Thickness.
In Reply to John at 20:19 Mar-23-2020 (Opening).

Hi John.

If your question is related to T-276.2 (a), in ASME V:

 -See the definitions for nominal thickness and weld
   reinforcement, in the applicable codes.

 -RT is not required in ASME VII.

 -For ASME B31.3. See the symbols "L" and "F" in the
tables 341.3.2 and K341.3.2, respectively.

 -For ASME IX. RT may be used for welder qualification or
  welding operator and, for these qualifications, the weld
  reinforcement is not considered; therefore this value
will be 0

 
 Reply 
 
John
John
14:04 Mar-25-2020
Re: ASME RAD Ref. Code Penetreted Thickness.
In Reply to Diego at 12:26 Mar-25-2020 .

Thanks for the information Diego.

I made a mistake, I meant VIII (section 8), not VII.

 
 Reply 
 
Diego
Consultant,
Freelance, Spain, Joined May 2013, 197

Diego

Consultant,
Freelance,
Spain,
Joined May 2013
197
14:37 Mar-25-2020
Re: ASME RAD Ref. Code Penetreted Thickness.
In Reply to John at 14:04 Mar-25-2020 .

If you use ASME VIII Div 1, you should consider UW-35 in general; but you should keep in mind that UW-35 may be modified by another paragraph of this division (as an example: see UHT 84)

 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window