where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

3653 views
Technical Discussions
S.R.G.PRABHU
NDT Inspector, AUT AUDITOR/ASNT LEVEL III/AWS SENIOR WELDING INS
India, Joined Sep 2004, 3

S.R.G.PRABHU

NDT Inspector, AUT AUDITOR/ASNT LEVEL III/AWS SENIOR WELDING INS
India,
Joined Sep 2004
3
08:27 Jan-01-2005
API RP 2X- TIPS

Someone please guide me in using API RP2X, with some practical tips in scanning ,T,K,Y joints.What is the normal procedure for passing a client's exam?To pass what is the minmum sizing of a mocked up defect?Is there any other points to note?I am aASNT LEVEL III in UT , but still have to qualify in TKY.
Prabhu


 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
00:13 Aug-02-2005
Re: API RP 2X- TIPS
----------- Start Original Message -----------
: Someone please guide me in using API RP2X, with some practical tips in scanning ,T,K,Y joints.What is the normal procedure for passing a client's exam?To pass what is the minmum sizing of a mocked up defect?Is there any other points to note?I am aASNT LEVEL III in UT , but still have to qualify in TKY.
: Prabhu
------------ End Original Message ------------

API RP 2X is a procedure that is "For information only" to guide engineers in the selection of NDT acceptance codes. If you want to have practical examples of T,K,Y inspection use AWS D1.1

Cheers



 
 Reply 
 
Ætheling
Ætheling
07:21 Aug-03-2005
Re: API RP 2X- TIPS
There's nothing new to it, RP2X has just one written test and it's the same with or without the T,K,Y certification.
The T,K,Y testing will be practical, in this one just remember, pay atention to the root configuration (do not believe the depth on the "digital" osciloscope), always try to draw the profile of the angles in a paper sheet to guide you trough the test. You can use a piece of lead and fold it following the contour of the pipes and welding.
Remember that the RP2X it's just a "recomended practice" but anyhow... some clients ask for it.


 
 Reply 
 

Product Spotlight

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>