Film Speeds

What film speeds does everyone usually use for iridium, cobalt and for x-ray. (ie; Kodak AA 1.8, Kodak T 2.5 , both when using Iridium). I would like to hear from as many people as possible and I will compile the results and post them here afterwards. You can email me at rt.film@sympatico.ca .

I think it would good idea if there was a guide for film speed selection based on actual indistry use and practice. So I would like to hear from the radiographers who actually use these numbers. I find the film speeds on the charts provided with the exposure calculators are not always what works best in the field.

I think this guide could help everyone.

Include any type and brand of film you like and say whether it is manual or automatic processing.

Thanks in advance guys!

rt.film@sympatico.ca


 
 Reply 
 
jeanne
Teacher
The Ocean Corp., USA, Joined May 2004, 2

jeanne

Teacher
The Ocean Corp.,
USA,
Joined May 2004
2
07:16 Mar-19-2004
Re: Film Speeds
---I've worked in RT for over 25 years and find that what works for me with Iridium Agfa D4 I use 4.5R, Agfa D7 I use 1.8 and Agfa D5 I use 3. With Kodak M I use 5.3R, T = 3 and AA = 1.8. It usually works well for me with manual processing
-------- Start Original Message -----------
: What film speeds does everyone usually use for iridium, cobalt and for x-ray. (ie; Kodak AA 1.8, Kodak T 2.5 , both when using Iridium). I would like to hear from as many people as possible and I will compile the results and post them here afterwards. You can email me at rt.film@sympatico.ca .
:
: I think it would good idea if there was a guide for film speed selection based on actual indistry use and practice. So I would like to hear from the radiographers who actually use these numbers. I find the film speeds on the charts provided with the exposure calculators are not always what works best in the field.
:
: I think this guide could help everyone.
: Include any type and brand of film youlike and say whether it is manual or automatic processing.
:
: Thanks in advance guys!
:
: rt.film@sympatico.ca
------------ End Original Message ------------




 
 Reply 
 
TU PHAM ANH
TU PHAM ANH
04:29 Jan-22-2005
Re: Film Speeds
Dear sir,

I've just being contacted with RT for 4 months. I'm colecting the system of film datas and factor of them in defferent film manufactorers.

I'm looking forward to receiving your respond!

Start Original Message -----------
: ---I've worked in RT for over 25 years and find that what works for me with Iridium Agfa D4 I use 4.5R, Agfa D7 I use 1.8 and Agfa D5 I use 3. With Kodak M I use 5.3R, T = 3 and AA = 1.8. It usually works well for me with manual processing
: -------- Start Original Message -----------
: : What film speeds does everyone usually use for iridium, cobalt and for x-ray. (ie; Kodak AA 1.8, Kodak T 2.5 , both when using Iridium). I would like to hear from as many people as possible and I will compile the results and post them here afterwards. You can email me at rt.film@sympatico.ca .
: :
: : I think it would good idea if there was a guide for film speed selection based on actual indistry use and practice. So I would like to hear from the radiographers who actually use these numbers. I find the film speeds on the charts provided with the exposure calculators are not always what works best in the field.
: :
: : I think this guide could help everyone.
: : Include any type and brand of film you like and say whether it is manual or automatic processing.
: :
: : Thanks in advance guys!
: :
: : rt.film@sympatico.ca
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window