NDE for helicopter rotor blades

Hello,
I've got a problem.
I have to come up with a in-service NDE system which should check 12 rotor blades per week.
My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.

I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.

Thanks for your advice,

Floriano.


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 304

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
304
02:56 Feb-07-2005
Re: NDE for helicopter rotor blades
----------- Start Original Message -----------
: Hello,
: I've got a problem.
: I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: Thanks for your advice,
: Floriano.
------------ End Original Message ------------


Dear Floriano,

NDT Consultants in the United Kingdom may be able to help you.

We have a research department, and they are just finishing a project looking at in-service (and in manufacturing) inspection of all types of Aerospace Composites.

One of the developments that has come our of this is N-BUS which we hope to have commercially available "within a few weeks". This is a C-Scan Narrow Band Ultrasonic Spectroscopy.

Alternatively, we are working with a research organisation in the USA developing an Ultrasonic Camera. This permits an almost real time (typically 1 to 2 seconds) image to be captured from immersion ultrasonics, covering an area of about 50mm x 50mm. They are also working on developments for larger areas of view, and also single sided inspection.

A third area is Digital Radiography, where very low X-Ray voltages can produce some high resolution X-Ray images.

Please get in touch with some more details, and we will see how we can cooperate with you.

Regards,

Godfrey Hands



 
 Reply 
 
Jens Forker
Jens Forker
02:17 Feb-07-2005
Re: NDE for helicopter rotor blades
Hello Floriano,

AE (acoustic emission) might be good tool for a check of the rotor blades. It requires loading of the blade but may provide a reasonable quick inspection of your blades.
If you are interested contact me for more information.
regards
Jens

----------- Start Original Message -----------
: Hello,
: I've got a problem.
: I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: I guess some ultrasonic technique, multi array probe forinstance, can do an overall good job but the whole process would be rather slow.
: Thanks for your advice,
: Floriano.
------------ End Original Message ------------




 
 Reply 
 
Jörg Collrep
Jörg Collrep
05:50 Feb-09-2005
Re: NDE for helicopter rotor blades
Hello Floriano,
have you ever tried to use Shearography for these tests. It might be worth to do this but it depends on the depth of the defects you are looking for. If you are interested in this technology or maybe would like to see a demo please contact me to discuss further details.
Rgds
Jörg


: : Hello,
: : I've got a problem.
: : I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: : My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: : I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: : I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: : I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: : Thanks for your advice,
: : Floriano.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
02:54 Feb-13-2005
Re: NDE for helicopter rotor blades
----------- Start Original Message -----------
: : Hello,
: : I've got a problem.
: : I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: : My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: : I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: : I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: : I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: : Thanks for your advice,
: : Floriano.
:
: Dear Floriano,
: NDT Consultants in the United Kingdom may be able to help you.
: We have a research department, and they are just finishing a project looking at in-service (and in manufacturing) inspection of all types of Aerospace Composites.
: One of the developments that has come our of this is N-BUS which we hope to have commercially available "within a few weeks". This is a C-Scan Narrow Band Ultrasonic Spectroscopy.
: Alternatively, we are working with a research organisation in the USA developing an Ultrasonic Camera. This permits an almost real time (typically 1 to 2 seconds) image to be captured from immersion ultrasonics, covering an area of about 50mm x 50mm. They are also working on developments for larger areas of view, and also single sided inspection.
: A third area is Digital Radiography, where very low X-Ray voltages can produce some high resolution X-Ray images.
: Please get in touch with some more details, and we will see how we can cooperate with you.
: Regards,
: Godfrey Hands
------------ End Original Message ------------

Dear Friend,

You can contact NDT Solutions at UK. They have a real time UT system called Rapidscan - which may be suitable to the application mentioned and you can do the scanning very fast. The data gives A scan, B Scan & C Scan of the component.

Contact Mr. Chris Kirby for more details.

Regards.
Amallraja.


 
 Reply 
 
agni
agni
09:43 Aug-25-2005
helicopter rotor blades
give some specifications to build the toy helicopter rotor blades


 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window