NDE for helicopter rotor blades

Hello,
I've got a problem.
I have to come up with a in-service NDE system which should check 12 rotor blades per week.
My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.

I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.

Thanks for your advice,

Floriano.


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
02:56 Feb-07-2005
Re: NDE for helicopter rotor blades
----------- Start Original Message -----------
: Hello,
: I've got a problem.
: I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: Thanks for your advice,
: Floriano.
------------ End Original Message ------------


Dear Floriano,

NDT Consultants in the United Kingdom may be able to help you.

We have a research department, and they are just finishing a project looking at in-service (and in manufacturing) inspection of all types of Aerospace Composites.

One of the developments that has come our of this is N-BUS which we hope to have commercially available "within a few weeks". This is a C-Scan Narrow Band Ultrasonic Spectroscopy.

Alternatively, we are working with a research organisation in the USA developing an Ultrasonic Camera. This permits an almost real time (typically 1 to 2 seconds) image to be captured from immersion ultrasonics, covering an area of about 50mm x 50mm. They are also working on developments for larger areas of view, and also single sided inspection.

A third area is Digital Radiography, where very low X-Ray voltages can produce some high resolution X-Ray images.

Please get in touch with some more details, and we will see how we can cooperate with you.

Regards,

Godfrey Hands



 
 Reply 
 
Jens Forker
Jens Forker
02:17 Feb-07-2005
Re: NDE for helicopter rotor blades
Hello Floriano,

AE (acoustic emission) might be good tool for a check of the rotor blades. It requires loading of the blade but may provide a reasonable quick inspection of your blades.
If you are interested contact me for more information.
regards
Jens

----------- Start Original Message -----------
: Hello,
: I've got a problem.
: I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: I guess some ultrasonic technique, multi array probe forinstance, can do an overall good job but the whole process would be rather slow.
: Thanks for your advice,
: Floriano.
------------ End Original Message ------------




 
 Reply 
 
Jörg Collrep
Jörg Collrep
05:50 Feb-09-2005
Re: NDE for helicopter rotor blades
Hello Floriano,
have you ever tried to use Shearography for these tests. It might be worth to do this but it depends on the depth of the defects you are looking for. If you are interested in this technology or maybe would like to see a demo please contact me to discuss further details.
Rgds
Jörg


: : Hello,
: : I've got a problem.
: : I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: : My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: : I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: : I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: : I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: : Thanks for your advice,
: : Floriano.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
02:54 Feb-13-2005
Re: NDE for helicopter rotor blades
----------- Start Original Message -----------
: : Hello,
: : I've got a problem.
: : I have to come up with a in-service NDE system which should check 12 rotor blades per week.
: : My rotor blade is made by a leading edge of solid CFRP with heater strip and erosion shield adhesively bonded. The rest of the structure is a non-metallic honeycomb (Nomex) with GFRP layers.
: : I have to detect delaminations on the solid CFRP; disbonds between CFRP, heater strip and erosion shield; and finally skin-core disbonds and region of crushed core.
: : I'm concerned due to the fact low frequency methods tend to work quite well with honeycomb and composite skins. But for the monolithic CFRP?
: : I guess some ultrasonic technique, multi array probe for instance, can do an overall good job but the whole process would be rather slow.
: : Thanks for your advice,
: : Floriano.
:
: Dear Floriano,
: NDT Consultants in the United Kingdom may be able to help you.
: We have a research department, and they are just finishing a project looking at in-service (and in manufacturing) inspection of all types of Aerospace Composites.
: One of the developments that has come our of this is N-BUS which we hope to have commercially available "within a few weeks". This is a C-Scan Narrow Band Ultrasonic Spectroscopy.
: Alternatively, we are working with a research organisation in the USA developing an Ultrasonic Camera. This permits an almost real time (typically 1 to 2 seconds) image to be captured from immersion ultrasonics, covering an area of about 50mm x 50mm. They are also working on developments for larger areas of view, and also single sided inspection.
: A third area is Digital Radiography, where very low X-Ray voltages can produce some high resolution X-Ray images.
: Please get in touch with some more details, and we will see how we can cooperate with you.
: Regards,
: Godfrey Hands
------------ End Original Message ------------

Dear Friend,

You can contact NDT Solutions at UK. They have a real time UT system called Rapidscan - which may be suitable to the application mentioned and you can do the scanning very fast. The data gives A scan, B Scan & C Scan of the component.

Contact Mr. Chris Kirby for more details.

Regards.
Amallraja.


 
 Reply 
 
agni
agni
09:43 Aug-25-2005
helicopter rotor blades
give some specifications to build the toy helicopter rotor blades


 
 Reply 
 

Product Spotlight

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window