bonding piezoelectric ceramics

I have some piezoelectric ceramic discs which i want to attach to a plate to do some work with lamb waves. However, the piezos have electrodes on each side of the disc and do not wrap round. Does anyone have any ideas on how to bond them properly to the plate.
Thanks
Cheryl


 
 Reply 
 
Joerg Schulze-Clewing
Joerg Schulze-Clewing
01:40 Mar-23-2004
Re: bonding piezoelectric ceramics
Cheryl, can you bond wire to the electrode, for example using
conductive epoxy and then glue them? As long as you don't
use high power levels this could work.

Regards, Joerg.

----------- Start Original Message -----------
: I have some piezoelectric ceramic discs which i want to attach to a plate to do some work with lamb waves. However, the piezos have electrodes on each side of the disc and do not wrap round. Does anyone have any ideas on how to bond them properly to the plate.
: Thanks
: Cheryl
------------ End Original Message ------------




 
 Reply 
 
Cheryl Forrester
Cheryl Forrester
01:46 Mar-23-2004
Re: bonding piezoelectric ceramics
would it be possible to use a conductive glue then use the plate as the 2nd electrode. I need to put three discs on the same plate so could this work?
Thanks
Cheryl

----------- Start Original Message -----------
: Cheryl, can you bond wire to the electrode, for example using
: conductive epoxy and then glue them? As long as you don't
: use high power levels this could work.
: Regards, Joerg.
: : I have some piezoelectric ceramic discs which i want to attach to a plate to do some work with lamb waves. However, the piezos have electrodes on each side of the disc and do not wrap round. Does anyone have any ideas on how to bond them properly to the plate.
: : Thanks
: : Cheryl
------------ End Original Message ------------




 
 Reply 
 
Robert Paynter
Robert Paynter
09:18 Mar-23-2004
Re: bonding piezoelectric ceramics
----------- Start Original Message -----------
... piezos have electrodes on each side of the disc and do not wrap round. Does anyone ...
------------ End Original Message ------------

I think you may need to get different piezo discs. Could you not get them attached to a foil on one
side, with one of the electrodes attached to the
foil? Here's a sounder like that.

0.15 GPB - that's pretty good price - I suspect
you will be able to get higher spec ones elsewhere
I suspect the foil/plate it's already attached to
maybe too thick (but maybe not)

Good Luck

Robert



 
 Reply 
 
Joerg Schulze-Clewing
Joerg Schulze-Clewing
00:15 Mar-23-2004
Re: bonding piezoelectric ceramics
Cheryl, you could probably do that. I don't know
your application. My work is medical (so we use PZT-5)
and glueing on a steel plate doesn't really work there
because you'll get a lot of ringdown in the near field,
and poor target resolution. But if you have a CW case
then I guess it won't matter. Just make sure stuff doesn't
corrode much.

Another concern is ground. Mostly I need to have the
front electrode grounded for noise immunity. In your
case that may not be possible because you want to glue
multiple transducers on the same steel plate. So then
the steel would be the common ground.

One other suggestion: You could also used copper clad
circuit board material if you need the back electrodes
of the three transducers separate. It's just not a very
good "backing material". But if you make the copper clad
larger than the transducers then you'd have a place to
solder your cable to.

Regards, Joerg.

----------- Start Original Message -----------
: would it be possible to use a conductive glue then use the plate as the 2nd electrode. I need to put three discs on the same plate so could this work?
: Thanks
: Cheryl
: : Cheryl, can you bond wire to the electrode, for example using
: : conductive epoxy and then glue them? As long as you don't
: : use high power levels this could work.
: : Regards, Joerg.
: : : I have some piezoelectric ceramic discs which i want to attach to a plate to do some work with lamb waves. However, the piezos have electrodes on each side of the disc and do not wrap round. Does anyone have any ideas on how to bond them properly to the plate.
: : : Thanks
: : : Cheryl
------------ End Original Message ------------




 
 Reply 
 
Klaus Brebøl
Klaus Brebøl
08:02 Mar-24-2004
Re: bonding piezoelectric ceramics
----------- Start Original Message -----------
: ... piezos have electrodes on each side of the disc and do not wrap round. Does anyone ...
: I think you may need to get different piezo discs. Could you not get them attached to a foil on one
: side, with one of the electrodes attached to the
: foil? Here's a sounder like that.
: 0.15 GPB - that's pretty good price - I suspect
: you will be able to get higher spec ones elsewhere
: I suspect the foil/plate it's already attached to
: maybe too thick (but maybe not)
: Good Luck
: Robert
------------ End Original Message ------------
If you are working at room temperature you can use the piezos you have. Changing temperatures can give problems, depending on geometry, due to difference in thermal expansion and a thin glue layer. Roughen the surface of the metal with emerycloth. Glue the parts together with a low viscosity glue (like water), epoxy or cyanoacrylate. Keep the parts under light pressure while curing. That will make electrical contact through the glue. Check the capacitance between top electrode on piezo and metal. If it is the same as for the piezo, contact is OK, if not then you have made a series connection of a piezo and a 'glue' capacitor. Cyano glue has the advantage that it dissolves in acetone, so you can try again.

Good luck

Klaus Brebøl





 
 Reply 
 
Cesar Quintero
Cesar Quintero
08:11 Feb-15-2005
bonding piezoelectric ceramics
This page is very important for my job. please, I need now how I can request a epoxic resin for a piezoelectric ceramic that stick to the aluminium piece for treatment medical in phisiotherapy?, thaks.


 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window