SAW and ERW pipes - standards

does anybody know of specific standards for UT of SAW and ERW pipes?
specificaly i am interested in the standards for inspection of the weld seam.


 
 Reply 
 
Ed T.
Ed T.
05:21 Sep-08-2004
Re: SAW and ERW pipes - standards
----------- Start Original Message -----------
: does anybody know of specific standards for UT of SAW and ERW pipes?
: specificaly i am interested in the standards for inspection of the weld seam.
------------ End Original Message ------------

Look in ASME Section V, Article 4 or 5. The basic calibration blocks for UT are based on the base material not the welding process.
However, the UT operator should be familiar with the welding process in order to determine what type of indications to excpect.


 
 Reply 
 
ajay singh
ajay singh
05:05 Feb-16-2005
Re: SAW and ERW pipes - standards
Dear sir,
we are looking for Stainless steel ERW or seam less pipe of AISI 304 or
310 grade.
outer dia 48.3 /44.5 thickness 2.6-2.7 MM length 6.1 Mt
Final destination Kolkata/Mumbai India.

Pls. offer your best price C&F destnation.Qunatity required is up to
200MT per month.
Regards,
ajay singh




 
 Reply 
 
Nikhil Arya
NDT Inspector
Surya Roshni Limited (Steel Division), India, Joined Jul 2005, 1

Nikhil Arya

NDT Inspector
Surya Roshni Limited (Steel Division),
India,
Joined Jul 2005
1
06:00 Jul-11-2005
Re: SAW and ERW pipes - standards
----------- Start Original Message -----------
: : does anybody know of specific standards for UT of SAW and ERW pipes?
: : specificaly i am interested in the standards for inspection of the weld seam.
: Look in ASME Section V, Article 4 or 5. The basic calibration blocks for UT are based on the base material not the welding process.
: However, the UT operator should be familiar with the welding process in order to determine what type of indications to excpect.
------------ End Original Message ------------

i can tell only for the ERW pipes. N10 & N5 notches at OD & ID are used and through holes at wels seam are used.


 
 Reply 
 
E Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

E Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
00:30 Jul-12-2005
Re: SAW and ERW pipes - standards
Standards for ERW and SAW pipe seam welds are similar world wide.
The North American versions are API 5L and in Canada CSA Z-245.
A Standard Practice by ASTM is also used, ASTM E-273.

Regards
Ed

----------- Start Original Message -----------
: : : does anybody know of specific standards for UT of SAW and ERW pipes?
: : : specificaly i am interested in the standards for inspection of the weld seam.
: : Look in ASME Section V, Article 4 or 5. The basic calibration blocks for UT are based on the base material not the welding process.
: : However, the UT operator should be familiar with the welding process in order to determine what type of indications to excpect.
: i can tell only for the ERW pipes. N10 & N5 notches at OD & ID are used and through holes at wels seam are used.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window