Re: ND Inspection of Resistance Spot Welds
: Dear sirs: I am interested to know if there are NDT
: which could be applied to on line resitance spot welding
: equipment, or to know some literature on this subject
: Thank you in advance
: Ricardo Rios-Jordana




 
 Reply 
 
kubilay dincer
kubilay dincer
08:33 Feb-10-2000
Re: ND Inspection of Resistance Spot Welds
: Dear sirs: I am interested to know if there are NDT
: which could be applied to on line resitance spot welding
: equipment, or to know some literature on this subject
: Thank you in advance
: Ricardo Rios-Jordana




 
 Reply 
 
narasimhan
narasimhan
06:18 Nov-19-2000
Re: ND Inspection of Resistance Spot Welds
dear sir i am doing project ndt of spot welding kindly send me details of books for reference for reference. iam having only soldidelay shoes how to do kindly send details


 
 Reply 
 
ali hasani
ali hasani
08:33 Jan-01-2001
Re: ND Inspection of Resistance Spot Welds
: Dear sirs: I am interested to know if there are ultrasonic method
: which could be applied to on line resitance spot welding
: equipment, or to know some literature on this subject
: Thank you in advance
: ali




 
 Reply 
 
ali hasani
ali hasani
00:35 Jan-01-2001
Re: ND Inspection of Resistance Spot Welds
: : Dear sirs: I am interested to know if there are NDT
: : which could be applied to on line resitance spot welding
: : equipment, or to know some literature on this subject
: : Thank you in advance
: : Ricardo Rios-Jordana

: Ricardo Rios-Jordana,

: We have to results available on NDTnet for which I copied below more details.

: The first one is an ultrasonic system called upi-50/SW which is manufactured
: by IRT Inc.
: (on NDTnet http://www.ndt.net/IRT or its Homepage http://www.irt.co.il)

: The second reference is an research summary from TWI of our abstract database.

: Our focus on UT/NDT of welding is planed for our April issue. During that
: month we would like to discuss this matter in depth. This month are other themes
: preferable to discuss here, especially is UT/NDT in Civil Engineering the TOPIC NOW.

: But don't hesitate to continue this topic on UT of Spot Weld.
: BTW: I heard that it might be a very difficult task for UT and
: UT companies were not successfully when they tried it years ago.

: Regards

: Rolf Diederichs

:
: ~~~~1~~~~
: http://www.irt.co.il/products/upi50sw/upi50sw.htm
: The upi-50/SW Series ultrasonic instrument provides the automotive industry
: with an easy-to-use, reliable means of inspecting and evaluating spot welds
: during production. Developed through continuous cooperation with the automobile
: industry, the upi-50/SW makes use of many of the outstanding features of our
: standard upi-50 ultrasonic instrument and application-oriented hardware and
: software tools.

: ~~~~2~~~~
: http://www.ndt.net/abstract/twi/005.htm
: Evaluation Of Ultrasonic And Electrical Resistance Methods For The
: Non-Destructive Testing (NDT) Of Resistance Spot Welds In Low Carbon Steel Sheet
: Author: By S.A. Westgate
: Number: 415

: MANAGEMENT SUMMARY 415/1990
: The work reported covers an extensive study of the non-destructive testing (NDT)
: of resistance spot welds in both laboratory madesamples and production
: components using conventional ultrasonic and electrical resistance measurements.
: Aspects of procedure development have been studied, followed by detailed testing
: of welds in uncoated low carbon steel sheet, with limited tests on zinc coated
: steel. Ultrasonic work included the assessment of various probe types and
: operating frequencies including attenuation studies. Investigation of the
: electrical resistance method covered an assessment of the factors influencing
: the measurements, such as impacting the welds prior to testing, edge distance
: and weld spacing and the distribution of voltage measurements across the weld.




 
 Reply 
 
a.hasani
a.hasani
09:00 Jan-17-2001
Re: ND Inspection of Resistance Spot Welds
: Dear sirs: I am interested to know if there are NDT
: which could be applied to on line resitance spot welding
: equipment, or to know some literature on this subject
: Thank you in advance
: Ricardo Rios-Jordana




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
00:04 Jan-17-2001
Re: ND Inspection of Resistance Spot Welds
You could look at the use of Acoustic Emission. On line manufacturing monitoring systems for spot welding of thin plate have been in use for many years particularly in the automotive industry. Resistance measurement might have some application as it is now proving very effective for production monitoring of laser welding on automotive car bodies





 
 Reply 
 

Product Spotlight

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window