Lining Thickness measurement

Dear Experts

Can the thickness of lining be measured in an internal cement lined pipe?

What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??

Thank you


 
 Reply 
 
Sasaki
Sasaki
08:28 Jul-22-2003
Re: Lining Thickness measurement
RT can be applicable to measure the thickness and the thickness uniformity of ganite lining of pipe inside.


 
 Reply 
 
Bijay Muduli
Engineering
IOCL, India, Joined Jul 2003, 4

Bijay Muduli

Engineering
IOCL,
India,
Joined Jul 2003
4
03:20 Aug-25-2003
Re: Lining Thickness measurement
I am inviting more opinions / (methods) on this subject.

Thanks & regards

B K Muduli


Dear Experts
.
: Can the thickness of lining be measured in an internal cement lined pipe?
.
: What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
.
: Thank you
.



 
 Reply 
 
David Castle
David Castle
05:12 Apr-02-2005
Re: Lining Thickness measurement
: Dear Experts
.
: Can the thickness of lining be measured in an internal cement lined pipe?
.
: What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
.
: Thank you
.

The thickness of cement lined pipe should be able to be measured using an eddy current device that is designed for the range of thicknesses that you are wanting to measure. I have used the Dinsearch DS500 for measuring Inconel cladding thickness in the range of 0 to 10 mm thickness with very good success. The company can be reached at:

Dinsley Devices Limited,
Ivy House, Streatlam Park,
County Durham, DL12 8TZ, UK.
Phone/Fax: +44 (0)1833 637971
email: dinsearch@hotmail.com

I hope that this is of help. Good Luck.
I hope that this may hekp you.



 
 Reply 
 
Charles Owston, Dinsley Devices Ltd
Charles Owston, Dinsley Devices Ltd
04:11 Apr-05-2005
Re: Lining Thickness measurement
----------- Start Original Message -----------
: : Dear Experts
: .
: : Can the thickness of lining be measured in an internal cement lined pipe?
: .
: : What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
: .
: : Thank you
: .
: The thickness of cement lined pipe should be able to be measured using an eddy current device that is designed for the range of thicknesses that you are wanting to measure. I have used the Dinsearch DS500 for measuring Inconel cladding thickness in the range of 0 to 10 mm thickness with very good success. The company can be reached at:
: Dinsley Devices Limited,
: Ivy House, Streatlam Park,
: County Durham, DL12 8TZ, UK.
: Phone/Fax: +44 (0)1833 637971
: email: dinsearch@hotmail.com
: I hope that this is of help. Good Luck.
: I hope that this may hekp you.
------------ End Original Message ------------

At Dinsley Devices Ltd we have over 25 years of experience in providing inovative solutions to problems in the inspection of pipes.

If you care to send details of your problem we will see if we can offer a solution.



 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window