05:39 Aug-26-2003
Detecting thermal crack by NDT methods

Dear All,
I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions


 
 Reply 
 
Bastiaan Janssen
NDT Inspector, Managing Xray micro-Tomography
NRG, Netherlands, Joined Jul 2003, 4

Bastiaan Janssen

NDT Inspector, Managing Xray micro-Tomography
NRG,
Netherlands,
Joined Jul 2003
4
03:13 Aug-27-2003
Re: Detecting thermal crack by NDT methods
Dear Velu Perumal,

Depending on size of test samples, erg. drilled core cylinders, I would suggest micro tomography,.Using x-ray or gamma ray's and a focal spot for the radiation source, this results in magnified projections wich can be reconstructed, using using many pictures form differend angeles, into a 3D-dataset. We have obtained internal crack visualisations of concrete cylinders diameter 5 cm, with a resolution of 1/10 m; Depending on x-ray energy, source spotsize and sample diameter...

Best regards.
(On holliday until october)
http://www.nrg-nl.com/product/ppt/tomo/index.html

----------- Start Original Message -----------
: Dear All,
: I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 
R.Malathy, Senior Lecturer in Civil Engineering, Kongu Engineering college, Peru
R.Malathy, Senior Lecturer in Civil Engineering, Kongu Engineering college, Peru
09:32 Feb-26-2004
Re: Detecting thermal crack by NDT methods
Dear Sir,

We have TICO ultrasonic Pulse velocity tester. How to measure the thermal cracks.


 
 Reply 
 
zuhudruba
zuhudruba
03:17 Apr-08-2005
Re: Detecting thermal crack by NDT methods
----------- Start Original Message -----------
: Dear All,
: I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 
TERD
TERD
08:21 Jul-03-2005
Re: Detecting thermal crack by NDT methods
----------- Start Original Message -----------
: Dear Velu Perumal,
: Depending on size of test samples, erg. drilled core cylinders, I would suggest micro tomography,.Using x-ray or gamma ray's and a focal spot for the radiation source, this results in magnified projections wich can be reconstructed, using using many pictures form differend angeles, into a 3D-dataset. We have obtained internal crack visualisations of concrete cylinders diameter 5 cm, with a resolution of 1/10 m; Depending on x-ray energy, source spotsize and sample diameter...
: Best regards.
: (On holliday until october)
: http://www.nrg-nl.com/product/ppt/tomo/index.html
: : Dear All,
: : I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window