Brian Hanni
Black & Veach, USA, Joined May 2001, 2

Brian Hanni

Black & Veach,
USA,
Joined May 2001
2
00:11 May-26-2005
Corrosion monitoring

My company is operating a facility whose processes involve a variety of highly toxic and corrosive chemicals. This facility has been in operation 10+ years. We are approaching a scheduled maintenance shutdown. During this extended shutdown we will have the opportunity to gain access to tank & piping systems that are normally very difficult to get to. We are looking for an inspection system that will provide corrosion profiles and ultimately provide service life information on these systems. The nature of the corrosion is localized corrosion cells on the inside. Ultrasonic thickness testing has proven to be ineffective due to scanning limitations. Misleading results occur as the transducer is placed next to but not over the corrosion cell.

Thank you for any suggestions.



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
01:08 May-26-2005
Re: Corrosion monitoring
----------- Start Original Message -----------
: My company is operating a facility whose processes involve a variety of highly toxic and corrosive chemicals. This facility has been in operation 10+ years. We are approaching a scheduled maintenance shutdown. During this extended shutdown we will have the opportunity to gain access to tank & piping systems that are normally very difficult to get to. We are looking for an inspection system that will provide corrosion profiles and ultimately provide service life information on these systems. The nature of the corrosion is localized corrosion cells on the inside. Ultrasonic thickness testing has proven to be ineffective due to scanning limitations. Misleading results occur as the transducer is placed next to but not over the corrosion cell.
: Thank you for any suggestions.
------------ End Original Message ------------


Dear Brian,
Sounds like a potential application for Ultrasonic Guideed Waves in conjunction with conventional Ultrasonic Scanning in the areas identified.

Ultrasonic Guided Waves are actually ultrasonic waves that propagate along a pipe (at a fairly low frequency) for up to 200 feet or more, and can detect significant corrosion (e.g. which represent somethjing in the order of 2 to 3% of the total pipe cross section. The distance from the sensor to this area of concern can then be identified, and this permits a detailed manual ultrasonic scanning to be planned for that specific area.
The testing can work underneath insulation (but some insuloation needs to be removed to allow access for the sensor).
It is best if you contact SwRI in San Antonio, Texas, who will be able to schedule some testing for you in the USA, either themselves or through one of their sub-contractors.
Please contact me first, and I will forward your message to them.

Godfrey Hands



 
 Reply 
 
Jim Knowles
Jim Knowles
01:13 May-26-2005
Re: Corrosion monitoring
----------- Start Original Message -----------
: My company is operating a facility whose processes involve a variety of highly toxic and corrosive chemicals. This facility has been in operation 10+ years. We are approaching a scheduled maintenance shutdown. During this extended shutdown we will have the opportunity to gain access to tank & piping systems that are normally very difficult to get to. We are looking for an inspection system that will provide corrosion profiles and ultimately provide service life information on these systems. The nature of the corrosion is localized corrosion cells on the inside. Ultrasonic thickness testing has proven to be ineffective due to scanning limitations. Misleading results occur as the transducer is placed next to but not over the corrosion cell.
: Thank you for any suggestions.
------------ End Original Message ------------

Brian
This is a case for tailoring a non destructive testing inspection technique to the problem. Obviously we know the problemswith direct contact of a transducer over the top of a corrosion pit and the inabilty to accurately measure the true under lying thickness or depth of flaw. In our systems we have used focused / stand off transducers in different arrangements coupled to short scanning systems to produce B & C scans. We then can see the profile of the corrosion pits. If as you state there are limtations in thescanning area, then look at radiographic means todays imaging systes can give corrosion profiles, similarly EC system give superb results once the inspection technique has been thoroughly tested for that application.


 
 Reply 
 
Richard Kazares
Richard Kazares
02:17 May-26-2005
Re: Corrosion monitoring
Our company (through Conam) can provide corrosion testing services using an EXTREMELY high speed scanning system known as the Large Structure Inspection (LSI) System. It is programmable - so the resolution can be tailored to the specific requirements of each application - and as scanning speeds are over 20 inches (1/2 Meter) per second - and data is captured as a C-Scan image (with numerical backup) - with ALL data retained for future reference - this might be the solution you are looking for.

I will send you some photos and video by direct e-mail.


----------- Start Original Message -----------
: My company is operating a facility whose processes involve a variety of highly toxic and corrosive chemicals. This facility has been in operation 10+ years. We are approaching a scheduled maintenance shutdown. During this extended shutdown we will have the opportunity to gain access to tank & piping systems that are normally very difficult to get to. We are looking for an inspection system that will provide corrosion profiles and ultimately provide service life information on these systems. The nature of the corrosion is localized corrosion cells on the inside. Ultrasonic thickness testing has proven to be ineffective due to scanning limitations. Misleading results occur as the transducer is placed next to but not over the corrosion cell.
: Thank you for any suggestions.
------------ End Original Message ------------




 
 Reply 
 
John Pursley
R & D
Envision Product Design, USA, Joined Oct 1999, 23

John Pursley

R & D
Envision Product Design,
USA,
Joined Oct 1999
23
03:34 May-27-2005
Re: Corrosion monitoring
----------- Start Original Message -----------
: : My company is operating a facility whose processes involve a variety of highly toxic and corrosive chemicals. This facility has been in operation 10+ years. We are approaching a scheduled maintenance shutdown. During this extended shutdown we will have the opportunity to gain access to tank & piping systems that are normally very difficult to get to. We are looking for an inspection system that will provide corrosion profiles and ultimately provide service life information on these systems. The nature of the corrosion is localized corrosion cells on the inside. Ultrasonic thickness testing has proven to be ineffective due to scanning limitations. Misleading results occur as the transducer is placed next to but not over the corrosion cell.
: : Thank you for any suggestions.
: Brian
: This is a case for tailoring a non destructive testing inspection technique to the problem. Obviously we know the problems with direct contact of a transducer overthe top of a corrosion pit and the inabilty to accurately measure the true under lying thickness or depth of flaw. In our systems we have used focused / stand off transducers in different arrangements coupled to short scanning systems to produce B & C scans. We then can see the profile of the corrosion pits. If as you state there are limtations in thescanning area, then look at radiographic means todays imaging systes can give corrosion profiles, similarly EC system give superb results once the inspection technique has been thoroughly tested for that application.
------------ End Original Message ------------

Brian,

We have a new system for internal corrosion inspection of pipelines. Take a look at http://cmosxray.com/PDFS/ScanTrack PL.pdf



 
 Reply 
 
jimmy
jimmy
01:51 Jun-05-2005
Re: Corrosion monitoring
----------- Start Original Message -----------
as discussed about corrosion monitoring with guided wave u can only detect corrosion from a pipe with minimum 10 meter length gul is good for long distance pipe to find internal and external corrosion also for my experiance its good for pipeline corrosion monitoring also for vessels and tanks you can go for automated ultrasonic it will give an exact result even the tank is with full internal corrosion for external corrosion u r eyes is best tool to detect, with AUT u can go for A,B and C scan also topview, if u want more clarification send mail to me i will come back to u coz. iam doing both job togeter and we got very good experiance in this job
regards
jimmy


 
 Reply 
 

Product Spotlight

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window