X-ray pipeline crawler

This morning I was ask by a colleague about a supplier for x-ray pipeline crawlers. I don't have any idea.
Could anybody help me. please?

Thank you

Rainer


 
 Reply 
 
Richard D. Roberts
Engineering, Executive Managment
Quest Integrity Group, USA, Joined Nov 1998, 78

Richard D. Roberts

Engineering, Executive Managment
Quest Integrity Group,
USA,
Joined Nov 1998
78
06:47 May-27-1999
Re: X-ray pipeline crawler



 
 Reply 
 
RICARDO SANTAMARIA
RICARDO SANTAMARIA
09:13 May-28-1999
Re: X-ray pipeline crawler
We are an Spanish inspection company, based in Madrid, with more than 20.000 km. of pipeline inspected with gamma and X-ray crawlers. We have also branches in some countries apart from Spain. Additionaly we have automatic ultrasound equipment for real time pipeline weld inspection. (very high inspection speed).
If you need any further information do not hesitate to contact us.

regards,

Ricardo Santamaria.




 
 Reply 
 
Mike Bunn
Mike Bunn
04:59 May-29-1999
Re: X-ray pipeline crawler
: This morning I was ask by a colleague about a supplier for x-ray pipeline crawlers. I don't have any idea.
: Could anybody help me. please?

: Thank you

: Rainer

Rainer
You may wish to contact Dave Russell of Russell Technologies in Edmonton, Alberta, Canada. Their
address is: Russell Technologies, 4909-75 Ave., Edmonton, Alberta, Canada, T6B 2S3.
Phone # 780-469-4461, Fax # 780-462-9378 and e-mail is
drussell@russelltech.com. Hope it helps.
Mike


 
 Reply 
 
Peter Simpson
Director,
Ashtead Technology Ltd, United Kingdom, Joined Oct 1999, 12

Peter Simpson

Director,
Ashtead Technology Ltd,
United Kingdom,
Joined Oct 1999
12
02:00 Jun-02-1999
Re: X-ray pipeline crawler
You could try JME Ltd at tel +44 1502 500969, fax +44 1502 511932, web site www.jme.co.uk

: This morning I was ask by a colleague about a supplier for x-ray pipeline crawlers. I don't have any idea.
: Could anybody help me. please?

: Thank you

: Rainer




 
 Reply 
 
Christine Blach
Christine Blach
00:36 Jun-27-2000
Re: X-ray pipeline crawler
Do you have any statistics or data on the reliability of such crawling devices? I would be particularly interested how frequently it happens, that such a crawler is stuck somewhere in the middle of the pipeline and cannot be retrieved without cutting out a section of the pipe.
Thanks for your answer
Christine


: We are an Spanish inspection company, based in Madrid, with more than 20.000 km. of pipeline inspected with gamma and X-ray crawlers. We have also branches in some countries apart from Spain. Additionaly we have automatic ultrasound equipment for real time pipeline weld inspection. (very high inspection speed).
: If you need any further information do not hesitate to contact us.

: regards,

: Ricardo Santamaria.




 
 Reply 
 
bcheggerud
bcheggerud
07:10 Sep-28-2000
Re: X-ray pipeline crawler
I have connections to several manufactures,may I help?


: This morning I was ask by a colleague about a supplier for x-ray pipeline crawlers. I don't have any idea.
: Could anybody help me. please?

: Thank you

: Rainer




 
 Reply 
 
rajeev chaudhari
NDT Inspector
offshore testing & inspection services (I) pvt ltd, India, Joined Dec 2000, 17

rajeev chaudhari

NDT Inspector
offshore testing & inspection services (I) pvt ltd,
India,
Joined Dec 2000
17
05:15 Sep-09-2001
Re: X-ray pipeline crawler
I have x-ray pipeline crawlers for inspection of weld joints useful for cross country pipeline. Let me know the exact requirement.

thanks

rajeev chaudhari



 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window