Kåre Johansson
Kåre Johansson
01:32 Mar-04-2003
Re: Material designation
: Dear Colleagues,
.
: At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
: I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.
.
:
: Best regards
.
: Ms. Rena Setjo
.
The nearest equivalent pipe materials in ASTM/ASME are:
15Mo3 A335 P1 but P1 har 0,5Mo while 15Mo3 has 0,3Mo
10CrMo9 10 A335 P22
St35.8 III A106 Grade A


 
 Reply 
 
rajeev chaudhari
NDT Inspector
offshore testing & inspection services (I) pvt ltd, India, Joined Dec 2000, 17

rajeev chaudhari

NDT Inspector
offshore testing & inspection services (I) pvt ltd,
India,
Joined Dec 2000
17
03:27 Mar-04-2003
Re: Material designation
Dear Ms. Rena Setjo,
Probabaly you are looking for ASTM Code equivalent for the three types of alloys you mentioned.

ST-35.8 ASTMA36
15Mo3 ASTM A335 P11
10CrMo910 ASTM A335 P22

Please check at your end and revert directly at email address otislab@vsnl.net.
Please note that this is NDT Forum.

Regards,

Rajeev Chaudhari


: : Dear Colleagues,
: .
: : At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
: : I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.
: .
: :
: : Best regards
: .
: : Ms. Rena Setjo
: .
: The nearest equivalent pipe materials in ASTM/ASME are:
: 15Mo3 A335 P1 but P1 har 0,5Mo while 15Mo3 has 0,3Mo
: 10CrMo9 10 A335 P22
: St35.8 III A106 Grade A
.



 
 Reply 
 
m.s.tripathi
m.s.tripathi
01:18 Aug-28-2004
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: : Sir,
: : Could you please provide me with chemical composition & physical properties for all EN-series EN31,EN24,EN19.
: yours
: Raj kumar prajapati
------------ End Original Message ------------




 
 Reply 
 
sampath
sampath
06:38 Dec-21-2004
Re: Material designation
Dear sir

en-19 specification and equalint material
please sent our mail

with kind regards

sampath


 
 Reply 
 
Jitendra
Jitendra
05:11 Jan-04-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: Sir,
: Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: Regards
: R.Shankar
------------ End Original Message ------------




 
 Reply 
 
K R trivedi
K R trivedi
05:54 Feb-25-2005
chemistry of 15Mo3
kindly give us the chemistry and physical property of 15Mo3 material and nearest ASTM plate material designation.

Thanks & regards
K R TRIVEDI
Chief Resident Surveyor
Baxcounsel Inspection Bureau Pvt.Ltd.
Baroda, Gujarat State, India


 
 Reply 
 
K R trivedi
K R trivedi
05:56 Feb-25-2005
chemistry of 15Mo3
kindly give us the chemistry and physical property of 15Mo3 material and nearest ASTM plate material designation.

Thanks & regards
K R TRIVEDI
Chief Resident Surveyor
Baxcounsel Inspection Bureau Pvt.Ltd.
Baroda, Gujarat State, India


 
 Reply 
 
K R Trivedi
K R Trivedi
05:56 Feb-25-2005
chemistry of 15Mo3
kindly give us the chemistry and physical property of 15Mo3 material and nearest ASTM plate material designation.

Thanks & regards
K R TRIVEDI
Chief Resident Surveyor
Baxcounsel Inspection Bureau Pvt.Ltd.
Baroda, Gujarat State, India


 
 Reply 
 
srinu
srinu
08:40 Mar-10-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: Sir,
: Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: Regards
: R.Shankar
------------ End Original Message ------------




 
 Reply 
 
shankar
shankar
08:43 Mar-10-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: Sir,
: Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: Regards
: R.Shankar
------------ End Original Message ------------




 
 Reply 
 
Santosh Raijade
Santosh Raijade
06:19 Apr-22-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: : Sir,
: : Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
Hardness Achieved
: : Regards
: : Santosh
------------ End Original Message ------------




 
 Reply 
 
RAJESH GAWANDE
RAJESH GAWANDE
01:20 May-21-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: : Sir,
: : Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: : Regards
: : R.Shankar
------------ End Original Message ------------




 
 Reply 
 
Deepak Sakore
Deepak Sakore
01:02 Jun-09-2005
Re: Material Composition Physical properties of EN19,EN354,EN8
----------- Start Original Message -----------
: : : Sir,
: : : Could you please provide me with chemical composition & physical properties for EN19,EN354,EN8/9.
: : : Regards
: : : Deepak Sakore
------------ End Original Message ------------




 
 Reply 
 
Deepak Sakore
Deepak Sakore
01:51 Jul-04-2005
Re: Material Composition Physical properties of EN19
----------- Start Original Message -----------
: Sir,
: Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: Regards
: Deepak Sakore
------------ End Original Message ------------




 
 Reply 
 
enno
enno
04:45 Jul-13-2005
Material designation
: Dear college,
at present i have been working in marketing engineer Probabaly i am looking for ASTM Code equivalent for the
:
: 15Mo3 din 17243
:
: Please check at your end and revert directly at email address enno@mail.daekyung.co.id
.
: Regards,
.
: enno
.
.
.
:


 
 Reply 
 
Andres Reutter
Andres Reutter
05:55 Jul-13-2005
Re: Material designation
Dear Sir:

I read your coments on the equivalent of DIN 15Mo3 as ASTM A335 P11 . In many cases I have found that the tube manufacturers have the equivalence of DIN 15Mo3 as ASTM A335 P1 Do you know what is the diference between P1 and P11?


Regards

Andres Reutter

: Dear Ms. Rena Setjo,
: Probabaly you are looking for ASTM Code equivalent for the three types of alloys you mentioned.
.
: ST-35.8 ASTMA36
: 15Mo3 ASTM A335 P11
: 10CrMo910 ASTM A335 P22
.
: Please check at your end and revert directly at email address otislab@vsnl.net.
: Please note that this is NDT Forum.
.
: Regards,
.
: Rajeev Chaudhari
.
.
.
:
: : : Dear Colleagues,
: : .
: : : At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
: : : I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.
: : .
: : :
: : : Best regards
: : .
: : : Ms. Rena Setjo
: : .
: : The nearest equivalent pipe materials in ASTM/ASME are:
: : 15Mo3 A335 P1 but P1 har 0,5Mo while 15Mo3 has 0,3Mo
: : 10CrMo9 10 A335 P22
: : St35.8 III A106 Grade A
: .
.



 
 Reply 
 
T.Rajasekar
T.Rajasekar
08:25 Jul-14-2005
Material Composition Physical properties of EN24
Sir,
Could you please provide me with chemical specification, mechanical specifications, hardening procedure and graph, blackening procedure and hot chrome plating procedure and graph for EN24.

Regards
T.Rajasekar



 
 Reply 
 
Aakash arora
Aakash arora
05:38 Jul-15-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: : : Sir,
: : : Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: : : Regards
: : : R.Shankar
------------ End Original Message ------------




 
 Reply 
 
R.S.Chavan
R.S.Chavan
08:30 Jul-18-2005
Re: Material Composition Physical properties of ,EN24,
----------- Start Original Message -----------
: : : Sir,
: : : Could you please provide me with chemical composition & physical properties for EN24,EN8.
: : : Regards
: : : R.S. Chavan
------------ End Original Message ------------




 
 Reply 
 
Ruchir
Ruchir
02:24 Jul-20-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: : : Sir,
: : : Could you please provide me with chemical composition & physical properties for EN19.
: : : Regards
: : : ruchir
------------ End Original Message ------------




 
 Reply 
 
sumit
sumit
00:55 Jul-20-2005
Re: Material Composition Physical properties of EN8
Dear Sir,
Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.


 
 Reply 
 
vijayan
vijayan
01:52 Jul-21-2005
Re: Material Composition Physical properties of EN8
----------- Start Original Message -----------
: Dear Sir,
: Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.
------------ End Original Message ------------

vijayan



 
 Reply 
 
syed amir
syed amir
05:23 Jul-27-2005
Re: Material Composition Physical properties of EN8
----------- Start Original Message -----------
: : Dear Sir,
: : Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.
: vijayan
------------ End Original Message ------------

Dear Sir,
Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.
Amir




 
 Reply 
 
K.RAJESHKANNA
K.RAJESHKANNA
07:33 Aug-23-2005
Re: Material Composition Physical properties of EN8
Dear Sir,
Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.

WHAT IS THE SUBSTITUTION MATERIAL FOR THIS EN8



 
 Reply 
 
irfan shaikh
irfan shaikh
06:45 Sep-02-2005
Re: Material Composition Physical properties of EN19, EN24, EN31
----------- Start Original Message -----------
: : Sir,
: : Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: : Regards
: : IRFAN SHAIKH
------------ End Original Message ------------




 
 Reply 
 
MUHIEDDIN OWEIMER
MUHIEDDIN OWEIMER
09:24 Nov-10-2005
Re: Material Composition Physical properties of EN8
----------- Start Original Message -----------
: Dear Sir,
: Please provide me with composition of the material EN-8 .Is it alloy or simply Mild steel.
: WHAT IS THE SUBSTITUTION MATERIAL FOR THIS EN8
------------ End Original Message ------------
MUHIEDDIN OWEIMER




 
 Reply 
 
D.K. Dalal
D.K. Dalal
06:53 Dec-02-2005
Re: Material Composition Physical properties of EN31,EN24,EN19
----------- Start Original Message -----------
: Sir,
: Could you please provide me with chemical composition & physical properties for EN31,EN24,EN19.
: Regards
: R.Shankar
------------ End Original Message ------------




 
 Reply 
 
santosh mishra
santosh mishra
11:13 Feb-10-2009
Re: Material Composition Physical properties of EN31,EN24,EN19
In Reply to srinu at 08:40 Mar-10-2005 .

equivalent material in indian standard of en31,en24, en19

 
 Reply 
 
Anup
Anup
10:02 Jun-01-2010
Re: Re: Material Composition Physical properties of EN31,EN24,EN19
In Reply to santosh mishra at 11:13 Feb-10-2009 .

Dear friends ,

to get information about EN 19 material visit below website:-


http://www.roymech.co.uk/Useful_Tables/Matter/Strength_st.htm

 
 Reply 
 
muralidhar.kk
muralidhar.kk
10:20 Jun-30-2010
Re: Material Composition Physical properties of EN31,EN24,EN19
In Reply to m.s.tripathi at 01:18 Aug-28-2004 .

go to google.com and type chemical composition of En 31

 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window