where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

I&T Nardoni Institute
A state-of-the-art company servicing the metal, mechanical, aeronautical and railway industrial sectors

4162 views
Technical Discussions
coriolius
coriolius
05:19 Sep-16-2005
Which standards should refer to when doing MT and UT

I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.

Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?

I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.



    
 
 
Arunachalam
Arunachalam
01:04 Sep-16-2005
Re: Which standards should refer to when doing MT and UT
-Dear,
please refer the material standard which will give you the "Inspection and testing standard for Visual, NDT, DT with procedures and acceptance creteria"
---------- Start Original Message -----------
: I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.
: Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?
: I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.
------------ End Original Message ------------




    
 
 
Ed T.
Ed T.
07:46 Sep-19-2005
Re: Which standards should refer to when doing MT and UT
I don't know about BS Standards, but you can take a look at ASTM SE-709 for MT and ASTM SA-388 for UT. They can be found in the back of ASME Section V.

----------- Start Original Message -----------
: I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.
: Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?
: I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.
------------ End Original Message ------------




    
 
 
coriolius
coriolius
03:57 Sep-21-2005
Re: Which standards should refer to when doing MT and UT
Which material standard? Do you mean the material standard published by the steel manufacturer?

----------- Start Original Message -----------
: -Dear,
: please refer the material standard which will give you the "Inspection and testing standard for Visual, NDT, DT with procedures and acceptance creteria"
: ---------- Start Original Message -----------
: : I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.
: : Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?
: : I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.
------------ End Original Message ------------




    
 
 
Arunachalam
Arunachalam
06:54 Sep-23-2005
Re: Which standards should refer to when doing MT and UT
Dear ,
All materials are manufacted based on a particular Country standard, Like ASTM or BS or JIS,
So ask the company for more details, like material manufactring standard ,number & Grade of the material which you are going to test.
they must have the Standard Book if not you have to get from outside to refer for testing standards

For example if you need to test ASTM A105 forging Bar , refer ASTM A105 standard which will give you all testing requirements and further refernce stadards to refer.
Hope U understand,
Regards
Arun
---------- Start Original Message -----------
: Which material standard? Do you mean the material standard published by the steel manufacturer?
: : -Dear,
: : please refer the material standard which will give you the "Inspection and testing standard for Visual, NDT, DT with procedures and acceptance creteria"
: : ---------- Start Original Message -----------
: : : I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.
: : : Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?
: : : I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.
------------ End Original Message ------------




    
 
 
N.Kuppusamy
Consultant, Level-III
United Testing Co. Pte Ltd, Singapore, Joined Jan 2003, 13

N.Kuppusamy

Consultant, Level-III
United Testing Co. Pte Ltd,
Singapore,
Joined Jan 2003
13
04:20 Sep-24-2005
Re: Which standards should refer to when doing MT and UT
Dear Coriolius,
Please refer to the following standards, I think this may be useful to you.

Standard Number: BS 5138:1974
Title: Specification for magnetic particle flaw inspection of finished machined solid forged and drop stamped crankshafts.

Standard Number: BS EN 10308:2002
Title: Non-destructive testing. Ultrasonic testing of steel bars

Standard Number: BS EN 10228-4:1999
Title: Non-destructive testing of steel forgings. Ultrasonic testing of austenitic and austenitic-ferritic stainless steel forgings


Standard Number: BS A 305:1994, ISO 7961:1994
Title: Bolts. Test methods


Standard Number: BS EN 10228-1:1999
Title: Non-destructive testing of steel forgings. Magnetic particle inspection

Standard Number: BS M 36:1970
Title: Method for ultrasonic testing of special forgings by an immersion technique using flat-bottomed holes as a reference standard

Standard Number: BS EN 10228-3:1998
Title: Non-destructive testing of steel forgings. Ultrasonic testing of ferritic or martensitic steel forgings

Standard Number: BS EN 10228-4:1999
Title: Non-destructive testing of steel forgings. Ultrasonic testing of austenitic and austenitic-ferritic stainless steel forgings

Best Regards,

N.Kuppusamy
----------- Start Original Message -----------
: Dear ,
: All materials are manufacted based on a particular Country standard, Like ASTM or BS or JIS,
: So ask the company for more details, like material manufactring standard ,number & Grade of the material which you are going to test.
: they must have the Standard Book if not you have to get from outside to refer for testing standards
: For example if you need to test ASTM A105 forging Bar , refer ASTM A105 standard which will give you all testing requirements and further refernce stadards to refer.
: Hope U understand,
: Regards
: Arun
: ---------- Start Original Message -----------
: : Which material standard? Do you mean the material standard published by the steel manufacturer?
: : : -Dear,
: : : please refer the material standard which will give you the "Inspection and testing standard for Visual, NDT, DT with procedures and acceptance creteria"
: : : ---------- Start Original Message -----------
: : : : I need to make MT and UT inspection to some steel components such as hollow shaft, high strength steel bolt (about M20x100), some small steel connecting shaft (about 20mm-dia x 80mm length), lever (30mm square section x 80mm length). The inspection is for surface and sub/surface cracks and flaws.
: : : : Which BS (or EN, ISO) standards should I refer to regarding the general testing guidelines, techniques and acceptance criteria?
: : : : I know there are BS and ISO standards for MT and UT inspection of welds, but I can't find the one for inspection of non-welded general material.
------------ End Original Message ------------




    
 
 
A.A.AMIRI
Consultant, NDT/QC/WELD INSPECTION
Iran, Joined Nov 2005, 20

A.A.AMIRI

Consultant, NDT/QC/WELD INSPECTION
Iran,
Joined Nov 2005
20
05:59 Oct-31-2005
Re: Which standards should refer to when doing MT and UT
----------- Start Original Message -----------
: Dear Friend,
In general purpose of material testing,you can use ASTM standard.But as per design code or service of equipments, you can select exact standard or specificatio.,



    
 
 

Product Spotlight

TVC awarded UKAS accreditation

TVC are delighted to finally announce we have been awarded UKAS accreditation for our calibration
...
laboratory. Laboratory accreditation to ISO/IEC 17025:2005 enables us to conduct the Electrical Verification of Ultrasonic Flaw Detection Equipment to BS EN 12668-1:2010. It has taken many months of hard work and we want to thank our staff for all their efforts during this massive undertaking.
>

FlexoFORM™

The FlexoFORM™ solution integrates flexible phased array probe technology in a scanner to solv
...
e the challenges that come with inspecting pipe elbows. When combined with a water column, this solution can be used to collect easy-to-interpret data on elbows with diameters ranging from 4.5 in. OD up to flat and offers many benefits.
>

I&T Nardoni

NDT, RESEARCH AND DEVELOPMENT OF NEW METHODOLOGY, TRAINING CENTER I&T NARDON INSTITUTE was idiated
...
in 1988 by Giuseppe Nardoni, now president and owner of the company, based on his multi-annual and international experience in the field of NDT.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window