Corrosion Mapping instrument for aerospace applications

Dear all,
We thank you for your expertise advice so far.
Now,we are looking for an instrument specially designed for corrosion mapping of aircraft fuselage, wings and other components.
Please contact me if you have this instrument available.
Your advice on instrument type selection and resource is also highly appreciated.
Best regards,
Nguyen Trong My (Dr.)
President,
Vietnam Inspection Services Co., Ltd
60 Vong Thi, Tay Ho, Hanoi
Tel: 84 4 8362117
Fax: 84 4 7537558
Email: visco_ndt@hn.vnn.vn



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
00:09 Sep-22-2005
Re: Corrosion Mapping instrument for aerospace applications
Dear Dr. Nguyen,

Corrosion measurement will be dictated by the aircraft Prime (such as Boeing etc), and the exact technique will depend upon the thickness and number of layers etc.

However, NDT Consultants Ltd. in the UK has a new NDT instrument just on the market. This is their "Freescan" instrument.

Freescan permits a 3 dimensional C-Scan (mapping) of any feature that can be measured through an Analog or Digital output from any NDT instrument, such as an Eddy Current or Ultrasonic Instrument.

This permits an accurate mapping of the corrosion, using your current instrument and probes. (Provided your current instrument has an Analog or Digital output).

You do not need to connect your probe to any cables, wires or arms, because it is tracked using optical sensors. All data can be returned to a computer either using USB or Bluetooth technology.

The range of the instrument is up to 7 metres, with a field of view of 70 degrees.
It has been designed with Aircraft inspection in mind.

Please contact me for more details, and we can supply a .PDF brochure to any interested parties.

Godfrey Hands

----------- Start Original Message -----------
: Dear all,
: We thank you for your expertise advice so far.
: Now,we are looking for an instrument specially designed for corrosion mapping of aircraft fuselage, wings and other components.
: Please contact me if you have this instrument available.
: Your advice on instrument type selection and resource is also highly appreciated.
: Best regards,
: Nguyen Trong My (Dr.)
: President,
: Vietnam Inspection Services Co., Ltd
: 60 Vong Thi, Tay Ho, Hanoi
: Tel: 84 4 8362117
: Fax: 84 4 7537558
: Email: visco_ndt@hn.vnn.vn
:
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Simon Amallraja
08:20 Sep-27-2005
Re: Corrosion Mapping instrument for aerospace applications
----------- Start Original Message -----------
: Dear all,
: We thank you for your expertise advice so far.
: Now,we are looking for an instrument specially designed for corrosion mapping of aircraft fuselage, wings and other components.
: Please contact me if you have this instrument available.
: Your advice on instrument type selection and resource is also highly appreciated.
: Best regards,
: Nguyen Trong My (Dr.)
: President,
: Vietnam Inspection Services Co., Ltd
: 60 Vong Thi, Tay Ho, Hanoi
: Tel: 84 4 8362117
: Fax: 84 4 7537558
: Email: visco_ndt@hn.vnn.vn
:
------------ End Original Message ------------

You can also contact Mr. Chris Kirby of NDT Solutions Ltd, UK. They make Rapidscan, which is widely used for Aircraft Applications.

www.ndtsolutions.com

D.Simon Amallraja.


 
 Reply 
 

Product Spotlight

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window