Denny Cochrane
Denny Cochrane
02:34 Jun-07-1999
High Speed NDT

Currently, we are using Magnetic Particle Inspection in our heat
treat operation for the detection of quench cracks in automotive
components. Currently, we use an operator to visually inspect
the part, with a less than 100% success rate.

I am looking for alternative (hopefully automated) NDT
techniques which would be able to perform the same function with
a better success rate.

The system would have to be able to cover an area of 0.16 m^2 in
roughly 9 seconds (scanning speed of 18000 mm^2/second).

Any suggestions would be appreciated.


 
 Reply 
 
William G. Klene
William G. Klene
01:35 Jun-08-1999
Re: Response, High Speed NDT
Mr. Cochrane

Could you send Moraine Valley Community College three
or four parts that contain the quench cracks. We have
worked with several Chicago area companies on related
projects. There is no fee. The school works on various
projects so our students can see what goes on the REAL
world of NDT.

Don't know if we can help you out, but are willing
to try. I am the director of the school's NDE
ASSOCIATE OF APPLICED SCIENCE degree program. Please
visit our web site at www.mv.cc.il.us/nde.

Send the parts to: MORAINE VALLEY COMMUNITY COLLEGE
NDE Department
10900 S. 88 Av
Palos Hills, IL 60465

ATT: William G. Klene
Department Manager



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
08:06 Jun-08-1999
Re: High Speed NDT
: Currently, we are using Magnetic Particle Inspection in our heat
: treat operation for the detection of quench cracks in automotive
: components. Currently, we use an operator to visually inspect
: the part, with a less than 100% success rate.

: I am looking for alternative (hopefully automated) NDT
: techniques which would be able to perform the same function with
: a better success rate.

: The system would have to be able to cover an area of 0.16 m^2 in
: roughly 9 seconds (scanning speed of 18000 mm^2/second).

: Any suggestions would be appreciated.

Danny (and others),
Godfrey Hands Ltd is the UK sales agent for several companies offering Resonant Inspection, specifically for testing automotive components.

These tests are whole body tests that evaluate the surface and internal integrity of components (Crack detection and inclusions) as well as detecting components with incorrect hardness in one test.
Tests take varying times, but generally between 1 and 10 seconds should be considered.

Please see our web pages for more information on Resonant Inspection. http://www.hands-ltd.demon.co.uk

Let me know also where you are located, and I can put you in touch with somebody more local to you than the United Kingdom.


 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>