EN Standard for wire IQI

Hi
Does anyone know which EN Standard covers/describes the wire iqi´s?


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
09:32 Nov-11-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: Hi
: Does anyone know which EN Standard covers/describes the wire iqi´s?
------------ End Original Message ------------

Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.

Regards
Uli Mletzko
MPA, University of Stuttgart
(Germany)




 
 Reply 
 
Kaveh
Kaveh
07:26 Nov-14-2005
Re: EN Standard for wire IQI
----------- Start Original Message -----------
: : Hi
: : Does anyone know which EN Standard covers/describes the wire iqi?s?
: Try EN 462-1 for the description of the wire IQI's and/or EN 1435 (welds) resp. EN 12681 (castings) for the wire IQ requirements.
: Regards
: Uli Mletzko
: MPA, University of Stuttgart
: (Germany)
------------ End Original Message ------------

Dear Uli
Detail of IQI construction in EN-462-5-1996.
EN 462-1-1994 shows typical construction details of one design.
Tables of acceptable wire diameters for different specimen thickness are given in EN 462-3, EN 462-4 and EN 1435-1997.
This type of IQI is shown in detail in EN 462-2-1994
Tables of IQI sensitivities for the IQI on the film side are included in EN 1453-1997 and EN 462-3-1997.

Regards
Kaveh Edalati


 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window